Zobrazeno 1 - 10
of 50
pro vyhledávání: '"R J, Müller"'
Publikováno v:
Polymer Degradation and Stability. 91:2486-2498
The degradation of several aliphatic and aromatic polyesters with lipases from Candida cylindracea (CcL) and Pseudomonas species (PsL) was investigated applying nanoparticles of the polymers. Nanoparticles (diameters 50 nm to 250 nm) of a particle co
Publikováno v:
Chemosphere. 44:289-299
The biological degradation behaviour of the aliphatic-aromatic copolyester Ecoflex was investigated with regard to the degree of degradation and the intermediates formed during the degradation process. The individual thermophilic strain Thermomonospo
Publikováno v:
Journal of Materials Chemistry. 8:61-64
Three new perylene-3,4-dicarboximide chromophores5a–c have been synthesized. They are characterized by high extinction coefficients and excellent thermal and photochemical stability. They display liquid crystallinity and exhibit several discotic ph
Publikováno v:
Polymer Degradation and Stability. 59:203-208
Aliphatic/aromatic copolyesters, especially those synthesized from butanediol, adipic acid and terephthalic acid, have been shown to represent biodegradable plastics of high commercial interest. Within a range of approx. 30–55 mol% terephthalic aci
Publikováno v:
Tetrahedron. 53:6847-6860
Little is known about benzoylperyleneimides 3 . Two new syntheses of 3 have been worked out, based on boronic acid and organotin intermediates, respectively. These mild methods allow the isolation of the uncyclized precursor 10 and the introduction o
Publikováno v:
The Journal of Chemical Physics. 106:24-34
Raman spectra of oligo-p-phenylenes, oligorylenes, and oligoacenes of different chain lengths have been obtained in the solid state and in solution. Among the properties studied, particular attention is devoted to frequency and intensity dispersion o
Publikováno v:
Lipid / Fett. 99:40-45
Synthetic, biodegradable aliphatic polyesters often do not provide optimal properties of application (e.g. melting point of polycaprolactone: 60°C). Material properties of such polyesters can be improved by introducing aromatic compounds into polyme
Publikováno v:
Journal of Environmental Polymer Degradation. 3:121-131
Establishing carbon balances has been proven to be an applicable and powerful tool in testing biodegradability of polymers. In controlled degradation tests at a 4-L scale with the model polymer poly(β-hydroxybutyrate) (PHB), it was shown that the de
Publikováno v:
Journal of Macromolecular Science, Part A. 32:851-856
For investigation of the microbial accessibility of polyesters based on 1,3-propanediol, a series of different polymer structures (homo, random, and block copolymers) were synthesized by polycondensation of terephthalic acid, adipic acid, sebacic aci
Publikováno v:
Ultraschall in der Medizin (Stuttgart, Germany : 1980). 17(4)
This study investigates the reliability of ultrasonographic screenings for detecting fetal malformations in pregnancy. The data from 1505 screening examinations of pregnant women who underwent routine checks at the Department of Obstetrics of the Uni