Zobrazeno 1 - 10
of 49
pro vyhledávání: '"Quanzhong Guo"'
Publikováno v:
Anti-Corrosion Methods and Materials. 69:490-498
Purpose The purpose of this paper is to investigate the interfacial conductivity and corrosion resistance of the Ni–P/Ti4O7 composite coating that is deposited on a carbon steel substrate as bipolar plates for proton exchange membrane fuel cells. D
Publikováno v:
Progress in Organic Coatings. 182:107611
Publikováno v:
Journal of The Electrochemical Society. 164:C269-C275
Publikováno v:
Construction and Building Materials. 270:121434
Electrochemical chloride removal (ECR) technique as an effective repair method has been applied to chloride-attacked concrete structures. This research studies the influence of different external electrical fields on the ECR treatment for reinforced
Publikováno v:
Corrosion Science. 111:436-445
The corrosion of three Fe-19Ni-21Cr- x Al ( x = 0, 2, 6 at.%) alloys was studied at 900 °C in 10% CH 4 /H 2 and 1.57% CH 4 /H 2 . All alloys followed complex kinetics. Addition of 2 at.% Al had a slight effect on the corrosion behavior, while that o
Publikováno v:
High Temperature Materials and Processes, Vol 35, Iss 4, Pp 353-359 (2016)
The oxidation behavior of Ti-5Al-2.5Sn and Ti-6Al-4V produced by hot isostatic pressing (HIP) has been studied at 650–850°C in air for 24 h. The oxidation kinetics of both alloys followed the parabolic law with good approximation, except for Ti-5A
Publikováno v:
RSC Advances. 6:39053-39062
This work reports that the filiform corrosion of a AZ31B Mg alloy can be inhibited by compact plasma electrolytic oxidation (PEO) under a transient self-feedback control mode. Corrosion protection of the C-PEO film was investigated through an immersi
Publikováno v:
Materials Letters. 260:126912
Biomaterial polyacrylamide (PAM) hydrogel was first studied for self-healing coatings of Mg alloys. In this work, a PAM gel with Ce4+ inhibitor was in-situ composited on the surface of micro-arc oxidation treated AZ31 Mg alloy. The results indicated
Publikováno v:
Corrosion Science. 100:579-588
The oxidation of the Fe-5Cr-5Si and Fe-10Cr-5Si alloys has been examined under 1 and 10 −20 atm O 2 at 700 °C. In all cases the Cr additions improved the oxidation resistance of the Fe-5Si alloy by forming protective external scales rich in Cr- an
Publikováno v:
Corrosion Science. 98:507-515
The authors acknowledge financial support by NSFC of China under the research projects (Nos. 50971129 and 51371183). Abstract The oxidation of three Fe-xSi alloys (x = 5, 9, 13 at.%) under 10−20 atm O2 at 800 °C formed in all cases SiO2 layers. Fo