Publikováno v:
Cement and Concrete Research. 35:2014-2017
Reported below are the results from a study aimed at mitigating the deleterious alkali–silica reaction by using perlite powder as an admixture. The expansion of mortar bars containing various amounts of silica fume (SF), expanded perlite, and natur
Publikováno v:
Cement and Concrete Research. 33:1825-1830
Expansion of mortar specimens prepared with an aggregate of mylonite from the Santa Rosa mylonite zone in southern California was studied to investigate the effect of different alkali ions on the alkali–silica reaction in concrete. The expansion te
Publikováno v:
Cement and Concrete Research. 33:1539-1542
The objective of this experimental study was to use ground clay brick (GCB) as a pozzolanic material to minimize the alkali-silica reaction expansion. Two different types of clay bricks were finely ground and their activity indices were determined. A
Publikováno v:
Cement and Concrete Research. 30:817-822
The reaction of silica particles in solutions saturated or supersaturated with respect to portlandite is observed by transmission soft X-ray microscopy, and a model for calcium silicate hydrate (C-S-H) growth is proposed which corresponds with the mo
Publikováno v:
Cement and Concrete Research. 31:825-827
The alkali–silica reaction (ASR) produces an expansive gel that may cause cracking and displacement in concrete structures. Steel microfibers ranging from 1% to 7% by volume of cement mortar were incorporated to reduce the expansion and cracking. A
Publikováno v:
Cement and Concrete Research. 33:933-934
Publikováno v:
ACI Materials Journal. 90
This paper presents the feasibility of using gamma ray computerized tomography (CT) to inspect reinforced concrete specimens. An objective was to verify the CT resolution in determining the size and location of voids and reinforcing bars. It is descr
Publikováno v:
Cement, Concrete and Aggregates. 16:57
Due to high cement contents and reduced heat capacity, high-strength lightweight concrete is often exposed to elevated curing temperatures. In the production of lightweight concrete the aggregate is often wetted before use, but sometimes dry aggregat
Publikováno v:
Cement, Concrete and Aggregates. 11:126
The morphology of air-entrained voids has been observed using the low-temperature scanning electron microscope (LTSEM). The entrained voids have been examined in cement paste specimens at an age of 5 min.
Publikováno v:
Cement, Concrete and Aggregates. 10:68
A comprehensive test program on the behavior of high-strength mortar under different conditions has been performed by studying the propagation of ultrasonic waves (compressional and shear) through 2-in. (0.051 m) cubes. The increase of the ultrasonic