Zobrazeno 1 - 10
of 41
pro vyhledávání: '"Peer Woizeschke"'
Autor:
Christian Diegel, Thorsten Mattulat, Klaus Schricker, Leander Schmidt, Thomas Seefeld, Jean Pierre Bergmann, Peer Woizeschke
Publikováno v:
Applied Sciences, Vol 13, Iss 18, p 10507 (2023)
Background. Spatter formation at melt pool swellings at the keyhole rear wall is a major issue for laser deep penetration welding at speeds beyond 8 m/min. A gas nozzle directed towards the keyhole, that supplies shielding gas locally, is advantageou
Externí odkaz:
https://doaj.org/article/92ec4d91e4d74274adea7cbada0f8677
Autor:
Ronald Pordzik, Peer Woizeschke
Publikováno v:
Applied Sciences, Vol 10, Iss 11, p 3951 (2020)
The formation of defects such as pores during deep-penetration laser welding processes is governed by the melt pool dynamics and the stability of the vapor capillary, also referred to as the keyhole. In order to gain an insight into the dynamics of t
Externí odkaz:
https://doaj.org/article/764a690b37b8441893bd2fc4218f3e82
Autor:
Till Leithäuser, Peer Woizeschke
Publikováno v:
Journal of Manufacturing and Materials Processing, Vol 3, Iss 4, p 83 (2019)
The wetting behavior in laser brazing can be designated as inconstant, caused largely by external process discontinuities such as the wire feeding. To reveal periodic melt pool propagation effects that occur during laser brazing of aluminum and for a
Externí odkaz:
https://doaj.org/article/f8516e40f6fc4d0ab73e685c311fb793
Autor:
Andreas Felsing, Peer Woizeschke
Publikováno v:
Journal of Manufacturing and Materials Processing, Vol 3, Iss 3, p 71 (2019)
The quality of welds, as well as the necessity of post-processing, is challenged by spatter generation during the laser keyhole welding process. In this study, the influence of the magnesium content on spatter behavior is studied for three aluminum a
Externí odkaz:
https://doaj.org/article/559f67bdd4ba4aae8b178ec29b660449
Autor:
Villads Schultz, Peer Woizeschke
Publikováno v:
Journal of Manufacturing and Materials Processing, Vol 2, Iss 4, p 78 (2018)
Keyhole laser welding experiments with 1.5 mm thick aluminum sheets (EN AW-6082) were carried out with transversal beam oscillation and wire feeding. A circular cavity, which was named buttonhole, formed directly behind the laser spot at certain osci
Externí odkaz:
https://doaj.org/article/5dd6add2947d474d9284a0f5c4799304
Publikováno v:
Metals, Vol 7, Iss 12, p 535 (2017)
Wetting steel surfaces with liquid aluminum without the use of flux can be enabled by the presence of a zinc-coating. The mechanisms behind this effect are not yet fully understood. Research results on single aluminum droplets falling on commercial g
Externí odkaz:
https://doaj.org/article/3d9c59f44cf64f79bf9280dae3242d00
Autor:
Insa Henze, Peer Woizeschke
Publikováno v:
The International Journal of Advanced Manufacturing Technology. 125:679-687
Autor:
Won-Ik Cho, Peer Woizeschke
Publikováno v:
The International Journal of Advanced Manufacturing Technology. 119:6245-6254
In brazing, the interfacial conditions between the molten filler material and the solid workpiece are important, yet they cannot be observed experimentally. A two-dimensional axisymmetric simulation was conducted to analyze the behavior of a single d
Publikováno v:
Procedia CIRP. 111:541-546
Autor:
Jun Zhang, Michaela Zeißig, Raik Dörfert, Frank Jablonski, Reinhold Kienzler, Jens Schumacher, Brigitte Clausen, Peer Woizeschke, Frank Vollertsen
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::45914faf31543594e36edadefb19f661
https://doi.org/10.2139/ssrn.4428593