Zobrazeno 1 - 10
of 61
pro vyhledávání: '"Pasi Peura"'
Publikováno v:
Results in Materials, Vol 16, Iss , Pp 100341- (2022)
AA7075 alloy is a high-strength aluminum alloy with properties enhanced by heat treatments. However, like most high-strength aluminum alloys, AA7075 is non-weldable, as it suffers from hot cracking when it is welded or additively manufactured with fu
Externí odkaz:
https://doaj.org/article/dfb88e0e36cb40129c2b511674a5af1a
Publikováno v:
Journal of Materials Research and Technology, Vol 15, Iss , Pp 6608-6623 (2021)
The characteristics of dynamic recrystallization (DRX) of a CoCrFeMnNi high–entropy alloy (HEA) was investigated via hot compression testing in the temperature range 950–1100 °C and at true strain rates of 10−2 and 10−1 s−1. The discontinu
Externí odkaz:
https://doaj.org/article/548915c64f9f41969c44e8a645d3e38f
Publikováno v:
Science and Technology of Advanced Materials, Vol 21, Iss 1, Pp 43-55 (2020)
Models describing the constitutive flow behaviour of a metallic material are desired for appropriate process design and realization of defect-free components. In this study, constitutive equations based on the hyperbolic-sinusoidal Arrhenius-type mod
Externí odkaz:
https://doaj.org/article/dd4b1f8f876347efb0a989955a1f34f5
Publikováno v:
Metals, Vol 9, Iss 8, p 887 (2019)
The intercritical annealing and isothermal bainitic processing response was studied for three Nb and V microalloyed Transformation-Induced Plasticity (TRIP)-assisted 980 MPa grade steels. Their mechanical and microstructural properties were compared
Externí odkaz:
https://doaj.org/article/a3e96f4c86524308870abfb1bf73b76a
Publikováno v:
Metals, Vol 9, Iss 3, p 373 (2019)
The quenching and partitioning response following intercritical annealing was investigated for three lean TRIP-type high-Al steel compositions. Depending on the intercritical austenite fraction following annealing, the steels assumed either a ferrite
Externí odkaz:
https://doaj.org/article/903a417aafb74960b9895f907eb9b0cf
Publikováno v:
Applied Sciences, Vol 9, Iss 5, p 1031 (2019)
The modern high strength steel plates have an excellent combination of strength and toughness based on micro-alloying and complex microstructure. Retaining this combination of properties in the weld zone is a major challenge for applications in high-
Externí odkaz:
https://doaj.org/article/ce9e7b9764984eb4b6c9113da597b626
Stainless steels are commonly used in hydraulic components where they may be sus-ceptible to cavitation erosion. In this study the cavitation erosion resistance of AISI 420-type stainless steel is examined after quenching and partitioning (Q&P) heat
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::3287a8d4ad0d0f00102ff11db5c5760a
https://trepo.tuni.fi/handle/10024/147929
https://trepo.tuni.fi/handle/10024/147929
Autor:
Shahroz Ahmed, Jani Penttilä, Jari Rämö, Mari Honkanen, Veli-Tapani Kuokkala, Olli Oja, Pasi Peura
Medium manganese steel grades heat treated with the quench and partition (Q&P) treatment have shown promising results of strength and formability, but the number of studies on high aluminum medium manganese Q&P steels still remains rather limited. Co
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::c9410cdfd4c33afda3f540dfe570393d
https://trepo.tuni.fi/handle/10024/142512
https://trepo.tuni.fi/handle/10024/142512
This study presents the characteristics of hot deformation behavior of a Al0.3CoCrFeNi high entropy alloy in the temperature and strain rate ranges of 1023–1423 K and 10–3–10 s–1, respectively. The constitutive flow behavior was modeled based
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::5ef9ccb3dbcf2b18620f26de0a1f9185
https://trepo.tuni.fi/handle/10024/141875
https://trepo.tuni.fi/handle/10024/141875
Publikováno v:
Materials Characterization. 197:112693
To establish the characteristics and kinetics of dynamic softening in a Al0.3CoCrFeNi high–entropy alloy (HEA), isothermal compression tests were carried out in a suitable temperature range of 1273–1423 K at 10−2 and 10−1 s−1 in accord with