Zobrazeno 1 - 10
of 13
pro vyhledávání: '"Olli-Ville Laukkanen"'
Autor:
Jean Michél Merkes, Tarushyam Mukherjee, Silvia Chiera, Olli‐Ville Laukkanen, Joerg Bruenke, Tim Brust, Francesco Tessarolo, Fabian Kiessling, Magnus Rueping, Srinivas Banala
Publikováno v:
Advanced Materials Interfaces, Vol 11, Iss 6, Pp n/a-n/a (2024)
Abstract During the COVID‐19 pandemic, the use of polypropylene fleece‐based personal protection equipment (PPE) increased significantly to over ten million tons. Typically, most PPEs are discarded after a single use, to prevent self‐infection
Externí odkaz:
https://doaj.org/article/82d94e7597be45e9903518a4eca77b0b
Autor:
Fabian Hagemans, Fabrizio Camerin, Nabanita Hazra, Janik Lammertz, Frédéric Dux, Giovanni Del Monte, Olli-Ville Laukkanen, Jérôme J. Crassous, Emanuela Zaccarelli, Walter Richtering
Publikováno v:
Hagemans, F, Camerin, F, Hazra, N, Lammertz, J, Dux, F, Del Monte, G, Laukkanen, O V, Crassous, J J, Zaccarelli, E & Richtering, W 2023, ' Buckling and Interfacial Deformation of Fluorescent Poly(N-isopropylacrylamide) Microgel Capsules ', ACS Nano, vol. 17, no. 8, pp. 7257-7271 . https://doi.org/10.1021/acsnano.2c10164
Hollow microgels are fascinating model systems at the crossover between polymer vesicles, emulsions, and colloids as they deform, interpenetrate, and eventually shrink at higher volume fraction or when subjected to an external stress. Here, we introd
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::81b21b99a3366011186c4c09a3f9c616
https://cris.vtt.fi/en/publications/46a997f3-efd5-49b7-abeb-58b918ab5d94
https://cris.vtt.fi/en/publications/46a997f3-efd5-49b7-abeb-58b918ab5d94
Publikováno v:
Rheologica Acta. 57:745-756
Physical aging is a ubiquitous phenomenon in glassy materials and it is reflected, for example, in the time evolution of rheological properties under isothermal conditions. In this paper, time-resolved rheometry (TRR) is used to characterize this tim
Publikováno v:
Journal of non-crystalline solids
In this experimental study, we explore the broadening of the glass transition in chemically and structurally complex glass-forming liquids (CGFLs) by means of thermal and rheological characterization techniques. Petroleum fluids with different levels
Publikováno v:
Rheologica acta
Rheological properties such as stiffness, elasticity, and viscosity are crucial parameters for the use of bitumen as a construction material. In bitumen oxidation studies, the increased viscosity has often been related to an increase in polar interac
The temperature dependence of the dynamics of glass-forming liquids can be characterized by the dynamic fragility (m) and apparent activation energy (Ea) at the glass transition temperature Tg. In this study, we derive analytical expressions that all
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::d803a95cae52c9e55035c9e2e6de8f89
https://aaltodoc.aalto.fi/handle/123456789/37368
https://aaltodoc.aalto.fi/handle/123456789/37368
Publikováno v:
Construction and building materials
Polymer modification is widely used to improve the engineering properties of bitumen, the most commonly used polymer modifier being styrene-butadiene-styrene (SBS) block copolymer. Although extensive studies have been performed on polymer modified bi
Publikováno v:
Rheologica acta
While extensive research efforts have been devoted to understand the dynamics of chemically and structurally simple glass-forming liquids (SGFLs), the viscoelasticity of chemically and structurally complex glass-forming liquids (CGFLs) has received o
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::a36047723002cd44fa852226963d8af1
https://aaltodoc.aalto.fi/handle/123456789/37289
https://aaltodoc.aalto.fi/handle/123456789/37289
Autor:
Olli-Ville Laukkanen
The rheological characterization of glass-forming liquids is challenging due to their extreme temperature dependence and high stiffness at low temperatures. This study focuses on the special precautions that need to be taken to accommodate high sampl
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::88b7624b1f3dbc65ef39c1f1f9341d33
https://aaltodoc.aalto.fi/handle/123456789/37272
https://aaltodoc.aalto.fi/handle/123456789/37272
Publikováno v:
Transportation Research Record: Journal of the Transportation Research Board. 2445:12-20
For more understanding about asphalt pavement deterioration in Finland, a premature failure of major arterial Ring Road II surface layers was investigated. Documentation of mix design (MD), construction, and material quality analysis, before and afte