Autor:
O. B. Berdnik, I. N. Tsareva
Publikováno v:
Voprosy Materialovedeniya. :45-53
The paper presents the results of a study of changes in the structure and strength properties of a heat-resistant nickel alloy after various periods of operation in a gas turbine engine. It is shown that after 25,000 hours of operation, irreversible
Publikováno v:
Inorganic Materials: Applied Research. 13:740-744
Publikováno v:
Welding International. 36:250-255
Publikováno v:
Voprosy Materialovedeniya. :65-73
The issues of ensuring the stability of the structural state and mechanical properties are very relevant for production in the manufacture of products, as well as for assessing their quality and extending the resource. The article presents the result
Publikováno v:
Voprosy Materialovedeniya. :115-127
When studying the high-temperature behavior of the heat-protective coating of zirconium dioxide, the method of laser heating has been tested. The coating was applied by the method of high-energy plasma spraying on the intermetallic sublayer of the Ni
Publikováno v:
Voprosy Materialovedeniya. :99-107
To solve the problem of increasing the adhesive-cohesive strength of multifunctional plasma coatings used to protect parts of power and machine building equipment from wear and corrosion, a ceramic coating of the Al2O3–Ni system, obtained from a po
Publikováno v:
Russian Metallurgy (Metally). 2021:386-391
The mechanism of fracture of the plasma thermal barrier coatings made of mixtures of zirconia and yttria (5.5 and 7%) powders in the form of solid and hollow spherical particles is studied by sclerometry. The fracture of the coatings is found to occu
Autor:
Yu. P. Tarasenko, S. V. Kirikov, L. A. Krivina, A. V. Gonchar, I. N. Tsareva, V. I. Kuzmin, E. N. Razov, O. B. Berdnik, V. V. Mishakin
Publikováno v:
Problems of strenght and plasticity. 83:265-275
With the use of special technological techniques (layer-by-layer spraying, air cooling and substrate temperature control), the technologically complex problem of applying plasma coatings of increased thickness with high adhesive strength has been sol
Publikováno v:
Physics and Chemistry of Materials Treatment. 4:25-30
The regularities of changes in the structure and phase composition of the thermal protective aluminide-nickel coating (Ni — 45 %; Al — 14 %; Co — 22 %; Cr — 18.9 %; Fe — 0.15 %; Nb — 0.14 %; Y — 0.09 %; Ca — 0.06 %; Mn — 0.01 %; C
Publikováno v:
Problems of strenght and plasticity. 83:207-219
Intensively operated modern technology requires the use of high-strength fasteners. The article presents the results of studies of the structure and physical and mechanical properties of the material of fastening elements (threaded hardware) in order