Catalysis Letters. 95:157-161
The effect of residual chlorine on the metal-catalyzed reaction of solid calcium oxide with a gas mixture of methane and water vapor (CaO + CH4 + 2H2O → CaCO3 + 4H2) is investigated at temperatures in the range 613–713 K, using solid samples of I
Publikováno v:
Catalysis Letters. 77:63-66
With noble metal catalysts (Pd, Pt, Rh, Ir) present, hydrogen is formed by the interaction of solid calcium oxide with gas mixtures of methane and water vapor, according to CaO + CH4 + 2H2O → CaCO3 + 4H2. Among the metals, Ir and Rh are so active t
Publikováno v:
Catalysis Letters. 58:119-122
A study of the hydrogenation of solid CaCO3 has shown that the addition of Pd and Ir catalysts causes a change in the gaseous product and, consequently, in the kinetics of the reaction. In the absence of catalyst, CO is formed at higher than 700 K wi
Publikováno v:
Berichte der Bunsengesellschaft für physikalische Chemie. 100:68-72
The effect of cold-working on hydrogen solubilities in the dilute region (α phase) has been investigated for Pd1-xNix(x≤0.2), Pd1-xPtx(x≤0.19), and Pd1-xNi(1/2)xAg(1/2)x(x≤0.2) alloys by measuring pressure-composition isotherms between 273 and
Publikováno v:
Scripta Metallurgica et Materialia. 30:643-647
The purpose of this communication is to determine whether the solubility enhancements for cold-worked Pd-Ni alloys increase or decrease with atom fraction of Ni. Substitutional Ni atoms contract and Pd lattice, in contrast to the lattice expansion re
Publikováno v:
Catalysis Letters. 23:237-243
The role of hydrogen in carbon deposition on Ni has been studied at H2/CO < 1 and 698 K by determining the respective rates of the carbon-forming reactions: (1) CO + H2 →-C + H2O and (2) 2CO → C + CO2. The steady-state rate of reaction (1) increa
Publikováno v:
ChemInform. 23
Publikováno v:
ChemInform. 24
Publikováno v:
ChemInform. 25
Publikováno v:
Berichte der Bunsengesellschaft für physikalische Chemie. 96:1477-1482
The effect of annealing temperature on hydrogen solubilities in the dilute region (α phase) has been investigated for cold-worked Pd-Ag alloys containing from 5 to 40 atomic % Ag by measuring pressure-composition isotherms between 273 and 348 K. The