We have previously reported that sequence-controlled copolyesters such as poly((ethylene diglycolate) terephthalate) (poly(GEGT)) showed higher melting temperatures than those of the corresponding random copolymers and high biodegradability in seawat
Externí odkaz:
https://doaj.org/article/8a0c7796ca474b48923f921305305e1a
Autor:
Lamya Zahir, Takumitsu Kida, Ryo Tanaka, Yuushou Nakayama, Takeshi Shiono, Norioki Kawasaki, Naoko Yamano, Atsuyoshi Nakayama
Publikováno v:
Life, Vol 11, Iss 1, p 43 (2021)
An innovative type of biodegradable thermoplastic elastomers with improved mechanical properties from very common and potentially renewable sources, poly(L-lactide)-b-poly(2-methyl-1,3-propylene glutarate)-b-poly(L-lactide) (PLA-b-PMPG-b-PLA)s, has b
Externí odkaz:
https://doaj.org/article/aaccc195b73b49a69b2212f2f844800f
Autor:
Yuushou Nakayama, Kazumasa Watanabe, Ryo Tanaka, Takeshi Shiono, Norioki Kawasaki, Naoko Yamano, Atsuyoshi Nakayama
Publikováno v:
International Journal of Molecular Sciences, Vol 21, Iss 10, p 3674 (2020)
Poly(ester amide)s are attracting attention because they potentially have excellent thermal and mechanical properties as well as biodegradability. In this study, we synthesized a series of novel poly(ester amide)s by introducing γ-aminobutyric acid
Externí odkaz:
https://doaj.org/article/b94f769c904849599c128233f074b30a
Autor:
Hiroto Yokaryo, Atsuyoshi Nakayama, Norioki Kawasaki, Naoko Yamano, Sayuri Ida, Yutaka Tokiwa
Publikováno v:
Chemistry Letters; Mar2024, Vol. 53 Issue 3, p1-4, 4p
Publikováno v:
Materials Chemistry and Physics. 303:127813
Publikováno v:
Polymer Degradation and Stability. 167:44-49
A biodegradable polymer–titanium dioxide (TiO 2 ) nanocomposite with antimicrobial activity by photooxidation of the composited TiO 2 under fluorescent light irradiation was investigated. Polyamide 4 (PA4)–visible-light-sensitive TiO 2 nanocompos
Publikováno v:
Polymer Degradation and Stability. 166:290-299
In order to utilize biodegradable polymers as a functional material, it is important to make the best use of their biodegradability. Biodegradation of aliphatic polyesters, such as PCL, PBSA and P3HB, in seawater was investigated. BOD test using seaw
Publikováno v:
Polymer Degradation and Stability. 166:230-236
Herein, we report on the aquatic degradation of polyamide (nylon) 4. Polyamide 4 (PA4) has previously been shown to degrade in natural environments such as activated sludge and soil, as well as in vivo (when subcutaneously implanted in the backs of r
Autor:
Riki Kataoka, Nobuhiko Takeichi, Norioki Kawasaki, Ryouji Inoue, Tetsu Kiyobayashi, Yoshimitsu Oda
Publikováno v:
Journal of Power Sources. 346:128-133
A surface-roughened clad (S-clad) current collector significantly extends the cycle-life of the lithium ion negative electrode composed of a silicon micropowder and an aqueous binder. The high tensile strength of the S-clad is also proved to be impor
Publikováno v:
Polymer Degradation and Stability. 137:281-288
We determined that polyamide 4 (PA4), which is easily degraded in the environment, is also degraded in vivo . We previously reported that PA4 was degraded by activated sludge. However, the potential biodegradability of PA4 in vivo has not been evalua