QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY. 20:363-368
The spatter is cooled during scattering by the air. So, many spatters change from the melt state to the solidification state. Spatter does not adhere to the base metal and peripheral equipment in the solidification state. But, the possibility of adhe
Publikováno v:
Welding International. 16:123-130
Publikováno v:
QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY. 19:269-277
In the arc welding, spatters attached around the bead of base metal. The adhered spatters lower the surface quality of the welding product. Therefore, it is very important to remove the spatters from the welding product. In general, wire brushes of b
Autor:
Sankei Hori, Nobuhiko Nishiwaki
Publikováno v:
Seikei-Kakou. 11:804-809
Autor:
Sankei Hori, Nobuhiko Nishiwaki
Publikováno v:
TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series C. 64:1836-1841
The thermal deformation of a machine tool is caused by the inner heat sources such as bearings, motors and so on, and the outer heat sources, such as the room temperature variation and so on. When the heat generation is pulse-wise or step-wise occurr
Publikováno v:
Welding International. 12:173-179
Summary In this paper we studied the loci (paths) and the velocities of scattering spatter in shielded metal arc (MMA) welding with high titanium oxide type electrodes. We examined only spatter that flew off at a right angle to the weld line and pass
Publikováno v:
Welding International. 12:851-858
Summary In CO2 gas-shielded arc welding, spatter is scattered and adheres to the base metal surface. The main factors affecting any difference in the bonding force remain obscure. This paper examines the bonding force of spatter adhering to the surfa
Publikováno v:
QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY. 15:247-253
In this paper we studied the loci and the velocities of scattering spatters in shielded metal arc welding with high titanium oxide type electrode. We examined only spatters that flew off in the right-angle direction to the weld line and passed throug
Publikováno v:
Transactions of the Japan Society of Mechanical Engineers Series C. 63:1391-1396