Materialwissenschaft und Werkstofftechnik
Materialwiss. Werkstofftech. 2022, 53, 440–448
Materialwiss. Werkstofftech. 2022, 53, 440–448
Jet engines of airplanes are designed such that in some components damage occurs and accumulates in service without being critical up to a certain level of damage. Since maintenance, repair, and component exchange are very cost-intensive, it is neces