Zobrazeno 1 - 10
of 841
pro vyhledávání: '"Nickel-base superalloys"'
Publikováno v:
Materials & Design, Vol 247, Iss , Pp 113416- (2024)
Additive manufacturing (AM) offers significant advantages in fabricating complex three-dimensional metallic components, which are traditionally difficult to fabricate using subtractive methods. However, the AM of nickel-base superalloys poses signifi
Externí odkaz:
https://doaj.org/article/a0df4375609844b2828bd61ee89b4416
Publikováno v:
In Acta Materialia 1 January 2025 284
Autor:
Giuseppe Barbieri, Francesco Cognini, Chiara de Crescenzo, Alessandra Fava, Massimo Moncada, Roberto Montanari, Maria Richetta, Alessandra Varone
Publikováno v:
Metals, Vol 14, Iss 1, p 124 (2024)
Ni-base superalloys are employed to produce parts of aeronautic engines, space vehicles and power plants. During the production process or lifetime of components, cracks may occur which affect their performance. Reliable repairs can be carried out th
Externí odkaz:
https://doaj.org/article/170cd4f7e70e4e6892d8a96384a5b371
Publikováno v:
Materials & Design, Vol 219, Iss , Pp 110792- (2022)
Understanding the microstructural evolution mechanisms in machining of advanced materials is essential to achieve excellent surface integrity levels within the manufacture of safety–critical components. However, as thermal and mechanical effects ar
Externí odkaz:
https://doaj.org/article/d5105096b2154c0f91f92405ebfcfcd4
Autor:
Yangping Li, Yangyi Liu, Sihua Luo, Zi Wang, Ke Wang, Zaiwang Huang, Haifeng Zhao, Liang Jiang
Publikováno v:
Journal of Materials Research and Technology, Vol 9, Iss 6, Pp 14467-14477 (2020)
In precipitation hardening metallic materials, the size and volume fraction of precipitation phases are regarded as primary microstructural parameters to control the strength instead of others. Why? In this research, a supervised learning approach wa
Externí odkaz:
https://doaj.org/article/a72a71e6d82e4bcab7284d0f38fe0482
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Autor:
John Boswell, Jonathan Jones, Nicholas Barnard, Daniel Clark, Mark Whittaker, Robert Lancaster
Publikováno v:
Materials & Design, Vol 205, Iss , Pp 109725- (2021)
The nickel-based superalloy Haynes 282 is a promising candidate material among the existing batch of aerospace alloys for manufacture via laser powder bed fusion (LPBF). LPBF Haynes 282 has a strong preference for epitaxial grain growth in the (001)
Externí odkaz:
https://doaj.org/article/08454a93110e4a599885f64ab07433d9
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.