High-temperature corrosion of pure Ni3Al and its alloyed (2.99 wt.%Ti) in Ar-0.2%SO2 gas environment
Publikováno v:
Journal of Materials Research and Technology, Vol 17, Iss , Pp 3055-3065 (2022)
In this work, the high-temperature corrosion behaviour of pure Ni3Al (P–Ni3Al) and alloyed (2.99 wt.%Ti) Ni3Al (Ti–Ni3Al) was investigated in Ar-0.2%SO2 gas at 900–1100 °C for up to 100 h. The corrosion kinetics of P–Ni3Al and Ti–Ni3Al rev
Externí odkaz:
https://doaj.org/article/167e5b1186b7495293f165d9a5569bae
Publikováno v:
Environmental Science and Pollution Research. 29:16503-16516
The insulation materials are used to reduce heat loss to/from the ducts with additional investment. This study introduces an air gap between insulation and duct surface to reduce the quantity of insulation. It uses lifecycle cost (LCC) analysis to de
Publikováno v:
Metals and Materials International. 27:3260-3268
A multilayered TiAlSiN thin film consisting of alternating nanocrystalline Ti(Si)N and Al(Si)N nanolayers was deposited on steel by arc ion plating. The film composition was 26Ti–16.3Al–1.2Si–56.50N in at%. The film was corroded at 800–1000
Publikováno v:
Korean Journal of Metals and Materials. 57:236-244
ASTM P91 steel (viz. 9Cr-1Mo steel) was hot-dip aluminized to form a ~70 μm thick coating, and was then corroded in N2/0.1%H2S gas for 50 h at 800 and 900 ℃, to study the effect of aluminizing on the corrosion resistance of P91 steel in highly cor
Publikováno v:
Environmental science and pollution research international. 29(11)
The insulation materials are used to reduce heat loss to/from the ducts with additional investment. This study aims to reduce this additional investment in the duct application by introducing an air gap between insulation and duct surface. It uses Li
Publikováno v:
Metals, Vol 6, Iss 11, p 291 (2016)
Fe-(9, 19, 28, 37) wt. %Cr alloys were corroded at 700 and 800 °C for 70 h under 1 atm of N2, 1 atm of N2/3.2%H2O mixed gas, and 1 atm of N2/3.1%H2O/2.42%H2S mixed gas. In this gas composition order, the corrosion rate of Fe-9Cr alloy rapidly increa
Externí odkaz:
https://doaj.org/article/c03fc72bd24b44b48d06c855b67100f9
Publikováno v:
Metals, Vol 6, Iss 7, p 169 (2016)
Plastic deformation and strain-induced martensite (SIM, α′) transformation in metastable austenitic AISI 304 stainless steel were investigated through room temperature tensile tests at strain rates ranging from 2 × 10−6 to 2 × 10−2/s. The am
Externí odkaz:
https://doaj.org/article/a1480600d0e242dfb3e0678b382af0db
Autor:
Muhammad Ali Abro, Dong Bok Lee
Publikováno v:
Metals, Vol 6, Iss 2, p 38 (2016)
High-temperature corrosion of carbon steel in N2/0.1% H2S mixed gas at 600–800 °C for 50–100 h was studied after hot-dipping in the aluminum molten bath. Hot-dipping resulted in the formation of the Al topcoat and the Al-Fe alloy layer firmly ad
Externí odkaz:
https://doaj.org/article/241d6a10e28a45a58a3bbfdb792c6fe8
Publikováno v:
Korean Journal of Metals and Materials. 56:350-359
When 2.25Cr-1Mo steel was hot-dip aluminized, a coating consisting of (Al-rich topcoat)/(Al13Fe4 layer)/(Al5Fe2 layer) formed. With increment of oxidation temperature, the transform of Al→Al13Fe4→Al5Fe2→AlFe→AlFe3→α-Fe(Al)→α-Fe ℃curre
Publikováno v:
Metals and Materials International. 24:507-515
The T92 steel plate was hot-dip aluminized, and oxidized in order to characterize the high-temperature oxidation behavior of hot-dip aluminized T92 steel. The coating consisted of Al-rich topcoat with scattered Al3Fe grains, Al3Fe-rich upper alloy la