Zobrazeno 1 - 10
of 13
pro vyhledávání: '"Maxim Ozerov"'
Autor:
Elena Gachegova, Denis Davydov, Sergey Mironov, Alexander Kalinenko, Maxim Ozerov, Sergey Zherebtsov, Oleg Plekhov
Publikováno v:
Metals, Vol 14, Iss 9, p 1045 (2024)
Laser shock peening (LSP) is a relatively novel and promising surface hardening method. An absorbing layer, which is needed to protect the specimen surface from undesirable thermal effects caused by laser irradiation, should be considered as one of m
Externí odkaz:
https://doaj.org/article/8aeacdd1436d423197bce9f679f36315
Autor:
Maxim Ozerov, Vitaly Sokolovsky, Nikita Yurchenko, Ilya Astakhov, Elizaveta Povolyaeva, Oleg Plekhov, Damir Tagirov, Nikita Stepanov, Sergey Zherebtsov
Publikováno v:
Metals, Vol 14, Iss 1, p 104 (2024)
The TiNbZr/(Ti, Nb)B metal matrix composite with 2.5 vol.% of borides was produced by vacuum arc melting. The composite was then cold-rolled to thickness strains of 10, 20, 50, or 80%. In the initial condition, the composite had a network-like micros
Externí odkaz:
https://doaj.org/article/50657b41acb8417ea780195eb4d5e88f
Autor:
Maxim Ozerov, Nikita Stepanov, Vitaly Sokolovsky, Ilya Astakhov, Margarita Klimova, Alexander Galtsev, Lujun Huang, Sergey Zherebtsov
Publikováno v:
Metals, Vol 13, Iss 11, p 1812 (2023)
A Ti-6.5Al-2Zr-1Mo-1V/TiB metal-matrix composite with 10.0 vol.% of TiB reinforcing fibers was produced using vacuum arc melting and compared with an unreinforced arc-melted Ti-6.5Al-2Zr-1Mo-1V alloy. The initial microstructure of the composite consi
Externí odkaz:
https://doaj.org/article/10b9ddf7dce142a5ab0fd6c0de59fd52
Autor:
Maxim Ozerov, Nikita Yurchenko, Vitaly Sokolovsky, Elena Nozdracheva, Evgeniya Panina, Sergey Nadezhdin, Nikita Stepanov, Sergey Zherebtsov
Publikováno v:
Metals, Vol 13, Iss 2, p 353 (2023)
Ti(50-x)Zr38NbxTa8Sn4 high-entropy alloys with x = 0, 10, and 20 at.% were produced by vacuum arc melting in a high-purity argon atmosphere. The initial microstructures consisted of equiaxial bcc grains with sizes of 115 ± 30 µm, 250 ± 60 µm, and
Externí odkaz:
https://doaj.org/article/57f9acd848854aa698ea223198a0c36c
Autor:
Aleksander Prokhorov, Aleksei Vshivkov, Oleg Plekhov, Nikolai Kashaev, Fedor Fomin, Maxim Ozerov, Sergey Zherebtsov
Publikováno v:
Metals, Vol 11, Iss 8, p 1198 (2021)
This work is devoted to the experimental investigation of the effect of laser shock peening (LSP) on the thermo-mechanical properties of metals. ARMCO iron was chosen as the model material for the study. Samples were subjected to LSP, and were tested
Externí odkaz:
https://doaj.org/article/49ef82dfdc5b4cc4bd94dca2a1046772
Autor:
Maxim Ozerov, Elizaveta Povolyaeva, Nikita Stepanov, Volker Ventzke, René Dinse, Nikolai Kashaev, Sergey Zherebtsov
Publikováno v:
Metals, Vol 11, Iss 3, p 506 (2021)
A Ti-15Mo/TiB metal–matrix composite was produced by spark plasma sintering at 1400 °C. The fractions of the elements in the initial powder mixture were 80.75 wt.% Ti, 14.25 wt.% Mo, and 5 wt.% TiB2. The initial structure of the synthesized compos
Externí odkaz:
https://doaj.org/article/73e6624a5d4243bb9ea7557c0b0a6fbe
Autor:
Sergey Zherebtsov, Maxim Ozerov, Elizaveta Povolyaeva, Vitaly Sokolovsky, Nikita Stepanov, Dmitry Moskovskikh, Gennady Salishchev
Publikováno v:
Metals, Vol 10, Iss 1, p 40 (2019)
A Ti-15Mo/TiB metal matrix composite was produced by the spark plasma sintering process at 1400 °C using a Ti-14.25 wt.% Mo-5 wt.% TiB2 powder mixture. The microstructure and mechanical properties of the composite were studied after non-isothermal r
Externí odkaz:
https://doaj.org/article/08ccd32f77f5419582442e33622c0dd6
Autor:
Sergey Zherebtsov, Maxim Ozerov, Margarita Klimova, Dmitry Moskovskikh, Nikita Stepanov, Gennady Salishchev
Publikováno v:
Metals, Vol 9, Iss 11, p 1175 (2019)
A Ti-15Mo/TiB titanium−matrix composite (TMC) was produced by spark plasma sintering at 1400 °C under a load of 40 MPa for 15 min using a Ti-14.25(wt.)%Mo-5(wt.)%TiB2 powder mixture. Microstructure evolution and mechanical behavior of the composit
Externí odkaz:
https://doaj.org/article/8066b1a7286744ae8a35cbac079a8a78
Publikováno v:
Metals, Vol 7, Iss 11, p 507 (2017)
Effect of high-pressure torsion (HPT) at 400 °C on microstructure and microhardness of a Ti/TiB metal–matrix composite was studied. The starting material was produced by spark plasma sintering of a mixture of a pure Ti and TiB2 (10 wt %) powders a
Externí odkaz:
https://doaj.org/article/d3a7f00de98e4fcfaa850fbbf9367216
Publikováno v:
Bulletin of the Siberian State Industrial University. 1:80-85