Autor:
Martin Guttmann, Neysha Lobo-Ploch, Heiko Gundlach, Frank Mehnke, Luca Sulmoni, Tim Wernicke, Hyun Kyong Cho, Katrin Hilbrich, Alexander Külberg, Matthias Friedler, Thomas Filler, Indira Käpplinger, Dennis Mitrenga, Christian Maier, Olaf Brodersen, Thomas Ortlepp, Ulrike Woggon, Sven Einfeldt, Michael Kneissl
AlGaN-based far ultraviolet-C (UVC) light emitting diodes (LEDs) with a peak emission wavelength below 240 nm typically show a long-wavelength tail at >240 nm that is detrimental to the use of the devices for skin-friendly antisepsis. We present the