In this study, hot deformation behavior of SP-700 titanium alloy was investigated by hot compression tests in the temperature range of 700-9508C and at strain rates of 0.001, 0.1, and 1 s-1. Final mechanical properties of the alloy (hot compressed at
Publikováno v:
Journal of Materials Engineering and Performance. 28:6525-6537
In this paper, the constitutive modeling and hot deformation behavior of SP-700 titanium alloy was investigated by performing isothermal hot compression tests in the temperature range of 700-950 °C and strain rates of 0.001, 0.1, and 1 s−1. The fl
Publikováno v:
International Journal of Materials Research. 109:1136-1145
Hot deformation behavior of the SP-700 alloy is studied through continuous and interrupted hot torsion testing carried out at 850 and 1 000 °C at different pass-strains and inter-pass times. The flow curves of SP-700 alloy showed the discontinuous y
Publikováno v:
Journal of Materials Engineering and Performance. 29:723-723
The three original authors have agreed that Seyed Mahdi Abbasi’s name should be removed from the article. The byline should read Amir Hossein Sheikhali, Maryam Morakkabati.
Publikováno v:
International Journal of Materials Research. 105:755-763
The flow behavior, mechanical and physical properties of alloy Fe-29 Ni-17 Co were studied using hot compression and hot rolling tests over the temperature range of 900 °C to1 200 °C and strain rates of 0.001 s−1 to 1 s−1. At temperatures below
Publikováno v:
Metallurgical and Materials Transactions A. 45:5201-5211
Hot compression tests were conducted on Ti-13V-11Cr-3Al beta-Ti alloy in the temperature range of 1203 K to 1353 K (930 °C to 1080 °C) and at strain rates between 0.001 and 1 s−1 The stress–strain curves showed pronounced yield point phenomena
Publikováno v:
International Journal of Materials Research. 104:1122-1127
The superplastic behavior of Ti-13V-11Cr-3Al alloy with beta single phase structure and average grain size of 220 μm was investigated. It was found that elongation increases with temperature at strain rates of 0.1 and 1 s−1. The optimum condition