Zobrazeno 1 - 6
of 6
pro vyhledávání: '"Marta Kianicova"'
Autor:
Michal Krbata, Robert Ciger, Marcel Kohutiar, Maria Sozańska, Maroš Eckert, Igor Barenyi, Marta Kianicova, Milan Jus, Nad’a Beronská, Bogusław Mendala, Martin Slaný
Publikováno v:
Materials, Vol 17, Iss 3, p 658 (2024)
In the original publication [...]
Externí odkaz:
https://doaj.org/article/1806e1faf4d64c69af6033980f38647b
Autor:
Michal Krbata, Robert Ciger, Marcel Kohutiar, Maria Sozańska, Maroš Eckert, Igor Barenyi, Marta Kianicova, Milan Jus, Naďa Beronská, Bogusław Mendala, Martin Slaný
Publikováno v:
Materials, Vol 16, Iss 14, p 5014 (2023)
The presented work deals with the investigation of mechanical tribological properties on Inconel 625 superalloy, which is welded on a 16Mo3 steel pipe. The wall thickness of the basic steel pipe was 7 mm, while the average thickness of the welded lay
Externí odkaz:
https://doaj.org/article/320996c9c0fe4b6aa07346a3da5ec130
Publikováno v:
Defect and Diffusion Forum. 422:45-49
The absorbed impact energy KV and the dynamic fracture toughness KId of the low-alloyed steel OCHN3MFA were measured in the respective temperature ranges 〈–40, 90〉 and 〈–60, –20〉 °C. The values of impact energy in the range of 〈14.1,
Autor:
Marianna Trebuňová, Daniel Kottfer, Karol Kyziol, Mária Kaňuchová, Dávid Medveď, Róbert Džunda, Marta Kianicová, Lukáš Rusinko, Alena Breznická, Mária Csatáryová
Publikováno v:
Materials, Vol 16, Iss 14, p 5044 (2023)
This article presents a comparative study of WC and CrC coatings deposited by the plasma-enhanced chemical vapor method using the hexacarbonyls of W and Cr as precursors. The measured thicknesses of the WC and CrC coatings are equal to ca. 1.5 µm. T
Externí odkaz:
https://doaj.org/article/3f10222aa6904115b5468fbdbf1842bc
Publikováno v:
Materials, Vol 14, Iss 19, p 5875 (2021)
The temperature dependence of tensile characteristics and fracture toughness of the standardly heat-treated low-alloyed steel OCHN3MFA along with three additionally heat-treated grades was experimentally studied. In the temperature range of ⟨−196
Externí odkaz:
https://doaj.org/article/046145e927504b3c909e41dcf68cf721
Autor:
Karel Slámečka, Petr Šesták, Tomáš Vojtek, Marta Kianicová, Jana Horníková, Pavel Šandera, Jaroslav Pokluda
Publikováno v:
Advances in Materials Science and Engineering, Vol 2016 (2016)
Results are given of a fractographic study of biaxial in-phase bending/torsion fatigue fractures in specimens made of nitrided steel and nickel-based superalloy with protective coatings (diffusion coatings and plasma-sprayed thermal barrier coatings)
Externí odkaz:
https://doaj.org/article/b2514909ce6e4fe2b6d89e58a0506de3