Zobrazeno 1 - 10
of 28
pro vyhledávání: '"Majid Mehrabi-Mazidi"'
Autor:
Majid Mehrabi Mazidi, Hossein Sharifi, Mir Karim Razavi Aghjeh, Leila Zare, Hossein Ali Khonakdar, Uta Reuter
Publikováno v:
ACS Applied Materials & Interfaces. 15:22445-22470
Publikováno v:
Iranian Polymer Journal. 32:23-36
Autor:
Hossein Sharifi, Majid Mehrabi‐Mazidi
Publikováno v:
Polymer International. 70:1701-1716
Publikováno v:
Journal of Composite Materials. 55:265-275
The effect of microstructural evolution with hydrophilic-nanosilica (SiO2) concentration, ranging from 0 to 5 wt%, on mechanical properties and deformation micromechanisms of PP/EPDM/SiO2 (80/20/x) ternary blend-nanocomposites was investigated. Morph
Publikováno v:
Polymer Bulletin. 77:3767-3794
Morphology, mechanical properties and fracture behavior of polypropylene/polyamide 6/ethylene polypropylene diene monomer graft maleic anhydride (PP/PA6/EPDM-g-MA) ternary blends containing various amounts of the EPDM-g-MA rubbery phase (from 0 to 9
Publikováno v:
International Polymer Processing. 33:553-563
The relaxation behavior of PMMA-PS core-shell particles in PP matrix was studied. The effects of composition and viscosity ratio of core and shell forming components on relaxation processes of PP/(PMMA+PS) 80/20 ternary blends were evaluated at three
Publikováno v:
Macromolecules. 51:4298-4314
The inherent shortcomings of polylactide (PLA) including brittleness, low glass transition temperature, and melt strength during processing were addressed through a facile melt blending of PLA with polybutadiene-g-poly(styrene-co-acrylonitrile) (PB-g
Publikováno v:
Polymer Testing. 67:380-391
The effect of poly(methyl methacrylate) (PMMA) content on the fracture resistance, failure mechanisms and micromechanical deformation of poly(lactic acid) (PLA)/polybutadiene-g-poly(styrene-co-acrylonitrile) (PB-g-SAN) blend was studied. The fracture
Publikováno v:
Engineering Fracture Mechanics. 191:65-81
Polypropylene (PP)-based ternary blends comprising 15 wt% polyamide 6 (PA6) and 15 wt% of either reactive or nonreactive ethylene-propylene-diene monomer (EPDM-g-MA or EPDM) rubber were prepared. A core–shell morphology was observed for reactive bl
Publikováno v:
Composites Science and Technology. 149:134-148
Effect of localization of multiwall carbon nanotube (MWCNT) on the fracture toughness and deformation mechanisms of un-vulcanized and dynamically vulcanized polypropylene/ethylene-propylene terpolymer/multiwall carbon nanotube (PP/EPDM/MWCNT) blend-n