Autor:
M.I. Patino, M.J. Baldwin
Publikováno v:
Nuclear Materials and Energy, Vol 40, Iss , Pp 101700- (2024)
An analytical model of helium-induced fuzz growth on heated tungsten (Patino et al., 2023) is expanded to include the effects of material exposure temperature via an Arrhenius relation and helium-induced sputtering. The expanded model is able to repl
Externí odkaz:
https://doaj.org/article/05e926c429614cd58fee867dd54fd57f
Autor:
M.J. Baldwin, D. Nishijima, M.I. Patino, G. Gunner, T. Lynch, F. Chang, M.J. Simmonds, A. Založnik, S. Moore, B. Schwendeman, R. Ciamacco, R.P. Doerner, G.R. Tynan
Publikováno v:
Nuclear Materials and Energy, Vol 39, Iss , Pp 101643- (2024)
Externí odkaz:
https://doaj.org/article/15aed6a59ff84b60b38253a82a8cd5ff
Publikováno v:
Nuclear Materials and Energy, Vol 39, Iss , Pp 101641- (2024)
Deuterium and helium plasma exposures on bulk TiB2 and ZrB2 samples were performed using the PISCES-RF linear plasma device. 40 and 90 eV deuterium ion plasma exposures were performed at 240 and 800 °C sample temperatures, and 80 eV helium ion plasm
Externí odkaz:
https://doaj.org/article/dfb6ccd25186499db6360e7ec568ee2e
Autor:
M.J. Baldwin, H. Zhang, A. Založnik, M.I. Patino, M.J. Simmonds, D. Nishijima, P.R. Carriere, G.R. Tynan, T. Horn
Publikováno v:
Nuclear Materials and Energy, Vol 39, Iss , Pp 101626- (2024)
Tungsten targets produced by the additive manufacturing (AM) method of electron-beam powder-bed fusion, or 3-D metal printing, are exposed to high flux D plasma in the Pisces-RF linear plasma device with the plasma-exposed surface normal to the AM bu
Externí odkaz:
https://doaj.org/article/a7a9f0be5f1f476fbbfdc8b6358124cc
Autor:
M.J. Baldwin, D. Nishijima, M.I. Patino, G. Gunner, T. Lynch, F. Chang, M.J. Simmonds, A. Založnik, S. Moore, B. Schwendeman, R. Ciamacco, R.P. Doerner, G.R. Tynan
Publikováno v:
Nuclear Materials and Energy, Vol 36, Iss , Pp 101477- (2023)
The helicon-plasma based-linear plasma-materials-interaction device, Pisces-RF is introduced. Steady-state plasma parameters in the target region are electron density up to ∼1019 m−3, electron temperature up to ∼10 eV, and ion flux up to ∼102
Externí odkaz:
https://doaj.org/article/5efb0e9110e34b3998745d645e3e74e4
Publikováno v:
Nuclear Fusion, Vol 64, Iss 12, p 124001 (2024)
Steady-state deuterium plasma exposures were performed on ultra-high temperature ceramics titanium diboride (TiB _2 ) and zirconium diboride (ZrB _2 ) using the PISCES-RF linear plasma device (LPD) as early screening for first wall, plasma-facing app
Externí odkaz:
https://doaj.org/article/e106a8488d37483ebc6e5aee91745ea2
Autor:
D. Nishijima, M. Tokitani, D. Nagata, T. Schwarz-Selinger, A. Založnik, F. Chang, R.P. Doerner, M.I. Patino, M.J. Simmonds, M.J. Baldwin, G.R. Tynan
Publikováno v:
Nuclear Fusion, Vol 64, Iss 6, p 068002 (2024)
We reply to the comment by Li et al (submitted to Nucl. Fusion with this response) on our recent paper Nishijima et al (2023 Nucl. Fusion 63 126003). In this response, we address the existence of an incident ion energy, E _i , threshold for the deute
Externí odkaz:
https://doaj.org/article/9c9c2b94b84b4ad49f2fe3bec117657a
Publikováno v:
Nuclear Materials and Energy, Vol 34, Iss , Pp 101384- (2023)
Ballistic helium transport in tungsten during fuzz growth was investigated to provide insight into the helium-induced nanostructuring process which adversely affects the near-surface properties of tungsten plasma-facing components. An analytical mode
Externí odkaz:
https://doaj.org/article/f954e264874c4efd8603d24fe4cbc3c2
Publikováno v:
Nuclear Materials and Energy, Vol 34, Iss , Pp 101371- (2023)
The annealing of ∼1 μm thick tungsten–deuterium co-deposit layers produced at 320 ± 25 K is found to induce changes in the desorptive release behavior and crystal structure. The changes in co-deposits were revealed by annealing in the temperatu
Externí odkaz:
https://doaj.org/article/94ef803925cd4f57b9885544e0a28492
Publikováno v:
Nuclear Materials and Energy, Vol 34, Iss , Pp 101331- (2023)
A temperature dependent study was performed on the helium retention in tungsten fuzz layers, in an attempt to provide further insight into the fuzz formation process and its relationship to the amount of trapped helium. Fuzz layers with thicknesses o