Autor:
Ł. Maj, Z. Fogarassy, D. Wojtas, A. Jarzębska, F. Muhaffel, A. Sulyok, A. Góral, M. Kulczyk, H. Çimenoğlu, M. Bieda
Publikováno v:
Scientific Reports, Vol 13, Iss 1, Pp 1-7 (2023)
Abstract Silver nanoparticle (Ag-NP) containing antibacterial micro-arc oxidation (MAO) coatings have already been synthesized over titanium-based materials via the MAO process employed in silver acetate (AgC2H3O2) containing electrolyte. However, th
Externí odkaz:
https://doaj.org/article/5b778a8228bf40ff83157f81200fdab6
Publikováno v:
Bioactive Materials, Vol 6, Iss 1, Pp 26-44 (2021)
The study is concerned with the mechanical properties of Zn and three Zn–Mg double alloys with Mg concentrations: 0.5%, 1.0% and 1.5% in the form of rods with a diameter of 5 mm as potential materials for use in biodegradable medical implants, such
Externí odkaz:
https://doaj.org/article/578156c9c22e492cb52ffc1f07de5dcf
Publikováno v:
Bulletin of the Polish Academy of Sciences: Technical Sciences, Vol 68, Iss No. 4 (i.a. Special Section on Advances in Electrical Power Engineering), Pp 903-911 (2020)
The presented results describe the effect of severe plastic deformation on the structure and mechanical properties of AA5083 and AA5754 alloys. Both materials were subjected to single hydrostatic extrusion (HE) and cumulative hydrostatic extrusion in
Externí odkaz:
https://doaj.org/article/e1fecbbfa64c4bce93d33649dcb2208e
Publikováno v:
Archives of Metallurgy and Materials, Vol vol. 64, Iss No 3, Pp 1051-1058 (2019)
The broad range applications of Ultra-Fine Grained metals is substantially limited by the lack of a welding method that allows them to be joined without losing the strong refinement of structure. From this point of view, the solid state welding proce
Externí odkaz:
https://doaj.org/article/fa5814412c0f490baa5b09de8cf2faa1
Publikováno v:
Bulletin of the Polish Academy of Sciences: Technical Sciences, Vol 67, Iss No. 4, Pp 709-717 (2019)
The study attempts to investigate the influence of severe plastic deformation (SPD in the hydrostatic extrusion (HE) process on the anisotropy of the structure and mechanical properties of the AA 6060 alloy. Material in isotropic condition was subjec
Externí odkaz:
https://doaj.org/article/cdfa0335876740efbce479f8a5561898
Publikováno v:
Advances in Materials Science and Engineering, Vol 2015 (2015)
The differences in the microstructure and texture of two Ni single crystals, with different initial orientations (100 and 110), and of polycrystalline nickel, before and after severe plastic deformation (SPD) produced by hydrostatic extrusion (HE), h
Externí odkaz:
https://doaj.org/article/aa3dc1388bf54c76b951e8c7c6900bef
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.