Publikováno v:
Engineering Failure Analysis. 18:2211-2221
Austenitic stainless steel tubes are used as furnace tubes in petrochemical industries mainly because of their corrosion resistance and mechanical strength. AISI 347 grade stainless steel is used as furnace heater tubes in the fractionator of hydrocr
Publikováno v:
Fusion Engineering and Design. 86:452-455
The joining behavior of 304SS and Cu joint is important for the component materials of the first wall and divertor in the International Thermonuclear Fusion Experiment Reactor (ITER). In this research, the joining of 304 stainless steel (SS) and pure
Publikováno v:
Engineering Failure Analysis. 18:1067-1075
Radiant tube conforming to ASTM A-200 T5 grade of steel and service exposed for 20 years from an oil refinery was investigated for health check and safety aspect. Microstructural study of the service exposed tube revealed a ferritic–martensitic str
Publikováno v:
Materials Science and Technology. 26:610-614
In the present investigation, transition joints were produced by soldering Sn–Ag–Cu and Sn–Ag– Cu–Mn alloys to Cu substrate. Microstructure and mechanical properties of the assemblies were determined in reflowed condition and after aging at
Publikováno v:
Materials Science and Engineering: A. 527:1395-1403
Intermetallic phases play a major role in the creep behavior of Mg alloys. The effects of intermetallic phases on the creep behavior of AZ91 alloy have been studied in the present investigation. Thermally stable and finer intermetallic phases such as
Publikováno v:
Journal of Colloid and Interface Science. 327:377-383
Spherical silica and zirconia mixed titania and pure titania samples were prepared in presence of cetyltrimethylammonium bromide (CTAB) through controlled hydrolysis of corresponding metal alcoxides. Effect of surfactant amount and calcinations tempe
Autor:
P K Roy, J Swaminathan, Raghubir Singh, Prabha Prasad, M K Gunjan, Krishna Gugloth, R N Ghosh
Publikováno v:
Engineering Failure Analysis. 15:723-735
Reformer furnace heater tubes made of cast austenitic alloy steels serve in the temperature range of 1073–1173 K and pressure around 3–4 MPa. Though the design life is about 100,000 h (∼11.4 years), premature failures within 3–8 years are mor
Autor:
T B Singh, Trilochan Mishra, Raghuvir Singh, M K Gunjan, A S Bhattacharyya, Shashi Kant Tiwari
Publikováno v:
Surface and Coatings Technology. 201:7582-7588
Sol–gel alumina coatings were deposited on medical grade stainless steel (AISI 316L) with an intermediate layer of silica by dip-coating method. The coatings obtained were homogeneous, crack-free and consisted of low crystalline γ-Al2O3 along with
Publikováno v:
Journal of Colloid and Interface Science. 330:243
Corrigendum Corrigendum to “Surfactant mediated synthesis of spherical binary oxides photocatalyst with enhanced activity in visible light” [J. Colloid Interface Sci. 327 (2008) 377–383] T. Mishra a,∗, J. Hait b, Noor Aman b, M. Gunjan c, B.