Publikováno v:
Journal of the American Ceramic Society. 78:865-873
The complex impedance of a CuO/ZnO oxide semiconductor heterocontact was studied by applying a dc bias voltage in a mixture of CO or H2 (4000 ppm) in air between 250° and 400°C. The frequency dependence of reactance showed a minimum peak, and the a
Publikováno v:
Sensors and Actuators B: Chemical. 25:383-387
The a.c. impedances of a CuO(Na)/ZnO heterocontact have been investigated under a d.c. bias voltage (−10 to + 10 V) in CO- and H 2 -containing atmospheres at 250°C. The reactance (imaginary component of the impedance) shows characteristic changes
Publikováno v:
Journal of the American Ceramic Society. 77:1961-1964
The impedance characteristics of a CuO/ZnO oxide semiconductor heterocontact were investigated to study a new method of gas identification. This was done by applying a dc bias voltage in atmospheres of air-balanced, flammable CO or H2 gas (4000 ppm).
Publikováno v:
Journal of the Ceramic Society of Japan. 102:810-817
To improve the gas selectivity for carbon monoxide from hydrogen, the complex impedance characteristics under DC bias voltages were studied on a pn semiconductor heterocontact comprised of 1mol%Na2O-added CuO (as a p-type semiconductor) and ZnO (as a
Publikováno v:
Japanese Journal of Applied Physics. 32:4296
The response time of the photorefractive effect in Bi12GeO20 was evaluated for the first time using nearly degenerate two-wave mixing. The result was analyzed in the context of the charge transport theory and the trap density was determined as N A=2.
Publikováno v:
Japanese Journal of Applied Physics. 32:4364
The mode of occurrence and the origin of cracking of lithium tetraborate (Li2B4O7) single crystals during growth have been investigated. The melt temperature dependence and the origin of crystal cracking have been explained in terms of activation ent
Publikováno v:
Japanese Journal of Applied Physics. 32:2762
Tuning of resonant characteristics, especially of resonant frequency, was studied on surface acoustic wave resonator, which was formed on a lithium tetraborate substrate and adhered to a poled piezoelectric ceramic element. The resonant frequency was
Publikováno v:
Japanese Journal of Applied Physics. 31:3205
The moving grating method was applied to a photorefractive Bi12SiO20 crystal in order to enhance the light amplification factor γ0 in the two-wave mixing process and the reflectivity R of the phase conjugate wave in the four-wave mixing process. It
Publikováno v:
Ferroelectrics. 94:73-80
The characteristics of the ferroelectric and the electro-optic properties was investigated on the transparent PLZT ceramics, which had a slim D-E loop. The coercive force Ec was 0.24 × 106 V/m and the remnant polarization Pr was 7.9 × 10−2 C/m2 f
Publikováno v:
Ferroelectrics. 49:265-272
Interconnected porous Pb (Zr0.53 Ti0.47)O3 ceramics, with controlled porosity up to 0.73, were prepared. The piezoelectric coefficient, 933, measured using a resonant method and a Berlincourt d33 meter increased as the porosity increased. The d33 and