Sukyoung Hwang, Hirokazu Kato, Kazuho Okada, Myeong-heom Park, Avala Lavakumar, Reza Gholizadeh, Hiroki Adachi, Masugu Sato, Nobuhiro Tsuji
Publikováno v:
Materials Research Letters, Vol 12, Iss 8, Pp 571-579 (2024)
Ultrafine-grained (UFG) high-Mn austenitic steel exhibited unusual discontinuous yielding on its stress-strain curve, characterized by a yield drop followed by a stress plateau, indicative of Lüders deformation. Utilizing the digital image correlati
Externí odkaz:
https://doaj.org/article/3e5cc0c1d025478f854fd00924ed41d2
Publikováno v:
Acta Agrobotanica, Vol 72, Iss 3 (2019)
We have isolated germacranolide-type sesquiterpene lactones with an α-methylene-γ-lactone moiety, dehydrocostus lactone (DHCL), costunolide, santamarine, and a novel compound denoted artabolide [3-hydroxy-4,6,7(H)-germacra-1(10),11(13)-dien-6,12-ol
Externí odkaz:
https://doaj.org/article/a2d0bc326e5a403e8938cbb342c50969
Publikováno v:
ISIJ International. 62:2081-2088
A typical hydrogen-related transgranular fracture, namely quasi-cleavage fracture, is usually accompanied by serrated markings on the resultant fracture surfaces in steels with body-centered cubic phases. The present paper investigated the microscopi
Publikováno v:
ISIJ International. 62:2089-2094
The present study investigated the hydrogen-related fatigue fracture under various test frequencies in low-carbon martensitic steel. In the hydrogen-charged specimen, although the number of cycles to failure decreased with decreasing test frequency,
Publikováno v:
Scripta Materialia. 234:115568
Autor:
Kazuho Okada, Akinobu Shibata, Taisuke Sasaki, Hisashi Matsumiya, Kazuhiro Hono, Nobuhiro Tsuji
Publikováno v:
Scripta Materialia. 224
This study challenged to improve the resistance against hydrogen embrittlement by increasing the concentration of carbon segregated at prior austenite grain boundary (PAGB), XPAGB, in low-carbon martensitic steels. The specimens with/without carbon s
Publikováno v:
International Journal of Hydrogen Energy. 46:37509-37517
This study investigated the hydrogen-related fatigue fracture in 2Mn-0.1C steel having a lath martensite microstructure. The presence of hydrogen significantly reduced the fatigue life. The transgranular surface was a main component in each stress ra
Publikováno v:
International Journal of Fatigue. 143
The present paper investigated characteristics of fatigue fracture behavior, particularly initiation stage of fatigue fracture (Stage I), in an as-quenched martensitic steel from microstructural and crystallographic points of view. The detailed cryst
Publikováno v:
SSRN Electronic Journal.
In this study, the deformation microstructure of hydrogen-charged ferritic-pearlitic 2Mn-0.1C steel was characterized using SEM-BSE, SEM-EBSD, TEM, and neutron diffraction. The microscopic mechanism of hydrogen-related quasi-cleavage fracture along t
Publikováno v:
Acta Materialia. 225:117549
In this study, the deformation microstructure of hydrogen-charged ferritic-pearlitic 2Mn-0.1C steel was characterized using SEM-BSE, SEM-EBSD, TEM, and neutron diffraction. The microscopic mechanism of hydrogen-related quasi-cleavage fracture along t