Publikováno v:
Materials Transactions, JIM. 38:28-36
Studies the fatigue behaviour of Al-7Si-0.3 Mg sand cast alloys at varying iron levels and with beryllium and manganese trace additions and when the alloy is stircast and extruded. From the stress (S)-number of cycles to failure (N)-(S-N) curves it i
Publikováno v:
Practical Metallography. 33:359-368
This paper concerns the optimization of electropolishing techniques which are in use to prepare metallographic specimens for microstructural observation. Process variables such as bath temperature, concentration of electrolyte, electrode distance etc
Publikováno v:
Materials Science Forum. :207-212
Publikováno v:
Materials Characterization. 33:99-112
Although the detrimental effect of iron on the mechanical properties of A1-7Si-0.3Mg alloy has been well established, studies on neutralizing this effect have been very few and in- conclusive. The $\beta$-phase $(FeSiAl_5)$, seen in the interdendriti
Publikováno v:
Scripta Metallurgica et Materialia. 31:267-271
Among the aluminum cast alloys, the precipitation hardenable Al-7Si-0.3Mg is perhaps the most widely used alloy. Iron is present as an impurity in this alloy, and an increase in iron content adversely affects the fracture toughness and other mechanic
Publikováno v:
Cast Metals. 6:189-198
The detrimental effect of iron impurity on the mechanical properties and fracture toughness of Al-7Si-0.3Mg alloy has been widely reported. It is also quite evident that Fe forms the intermetallic ...
Publikováno v:
Materials Science and Technology. 9:189-204
A review of the research work that has been carried out thus far relating the casting and heat treatment variables to the structure and mechanical properties of Al–7Si–Mg (wt-%) is presented here. Although specifications recommend a wide range of
Publikováno v:
Materials Science and Engineering: A. 151:1-10
A dynamic fracture toughness study on Al-7Si-0.3Mg casting alloy with cadmium trace addition and at varying magnesium and iron levels and solidification rates was carried out using an instrumented impact testing machine. With an increase in magnesium
Effect of Iron Impurity and a Cd Trace Addition on the Delayed Ageing of Al-7Si-0.3 Mg Casting Alloy
Publikováno v:
Cast Metals. 4:31-36
Publikováno v:
IndraStra Global.
Stirring an Al-7Si-0.3Mg casting alloy during solidification inhibits the creation of the dendritic structure such that the primary α-Al forms as spheroids and other compact irregular shapes owing to thixotropic behaviour. The extruded stir cast all