Autor:
Lei Zhang, Hanwen Liu, Bo Song, Jialun Gu, Lanxi Li, Wenhui Shi, Gan Li, Shiyu Zhong, Hui Liu, Xiaobo Wang, Junxiang Fan, Zhi Zhang, Pengfei Wang, Yonggang Yao, Yusheng Shi, Jian Lu
Publikováno v:
Nature Communications, Vol 15, Iss 1, Pp 1-14 (2024)
Abstract Continuous industrialization and other human activities have led to severe water quality deterioration by harmful pollutants. Achieving robust and high-throughput water purification is challenging due to the coupling between mechanical stren
Externí odkaz:
https://doaj.org/article/57e1c4bf29be43b5b1fbaa90f1db5bf6
Autor:
Shuaishuai Wei, Jinliang Zhang, Lei Zhang, Yuanjie Zhang, Bo Song, Xiaobo Wang, Junxiang Fan, Qi Liu, Yusheng Shi
Publikováno v:
International Journal of Extreme Manufacturing, Vol 5, Iss 3, p 032001 (2023)
NiTi alloys have drawn significant attentions in biomedical and aerospace fields due to their unique shape memory effect (SME), superelasticity (SE), damping characteristics, high corrosion resistance, and good biocompatibility. Because of the unsati
Externí odkaz:
https://doaj.org/article/34f53fb883e74162a8b1fd80875062f9
Autor:
Xiaobo Wang, Lei Zhang, Bo Song, Jinliang Zhang, Junxiang Fan, Zhi Zhang, Quanquan Han, Yusheng Shi
Publikováno v:
Acta Biomaterialia. 148:374-388
In bone scaffolds, the mechanical performance provides the load-bearing capability, and the mass-transport performance presented as permeability dominates the nutrients/oxygen transportation efficiency. Body-centered-cubic and face-centered-cubic pla
Autor:
Danlei Zhao, Changjun Han, Bo Peng, Tan Cheng, Junxiang Fan, Lei Yang, Lili Chen, Qingsong Wei
Publikováno v:
Acta biomaterialia. 153
Additively manufactured biodegradable zinc (Zn) alloy scaffolds constitute an important branch in orthopedic implants because of their moderate degradation behavior and bone-mimicking mechanical properties. This work investigated the corrosion fatigu
Publikováno v:
Journal of Materials Science & Technology. 68:35-39
In the present study, we offer an in-depth analysis over the microstructure, thickness and product composition of the interfacial reaction layer generated upon CBN/Cu-Sn-Ti active filler metal at 1223 K. Current findings demonstrate that adequate wet
Autor:
Zhi Zhang, Bo Song, Junxiang Fan, Xiaobo Wang, Shuaishuai Wei, Ruxuan Fang, Xinru Zhang, Yusheng Shi
Publikováno v:
Chinese Journal of Mechanical Engineering: Additive Manufacturing Frontiers. 2:100068
Publikováno v:
Metallurgical and Materials Transactions B. 51:880-884
Effects of different holding time on CBN/Cu-Sn-Ti composites have been thoroughly documented. It is revealed that adequate wetting can only take place at 30 minutes and beyond. The thickness of reaction layer is governed by Ti diffusion, and follows
Publikováno v:
Metallurgical and Materials Transactions B. 50:2517-2522
Cubic boron nitride (CBN)/Cu-Sn-Ti composites as potential superabrasive products are prepared. It is found that as the temperature increases, porosity keeps decreasing from 1123 K to 1223 K but becomes virtually constant afterward, which is inversel
Autor:
Xiaobo Wang, Lei Zhang, Bo Song, Zhi Zhang, Jinliang Zhang, Junxiang Fan, Shuaishuai Wei, Quanquan Han, Yusheng Shi
Publikováno v:
Composite Structures. 300:116172
Autor:
Junxiang Fan, Lei Zhang, Xiaobo Wang, Zhi Zhang, Shuaishuai Wei, Bo Song, Aiguo Zhao, Xiao Xiang, Xuefeng Zhu, Yusheng Shi
Publikováno v:
Chinese Journal of Mechanical Engineering: Additive Manufacturing Frontiers. 1:100036