João Paulo Mendes Tribst, Alison Flavio Campos dos Santos, Giuliane da Cruz Santos, Larissa Sandy da Silva Leite, Julio Chávez Lozada, Laís Regiane Silva-Concílio, Kusai Baroudi, Marina Amaral
Publikováno v:
Materials, Vol 14, Iss 18, p 5153 (2021)
This study tested whether three different cement layer thicknesses (60, 120 and 180 μm) would provide the same bonding capacity between adhesively luted lithium disilicate and human dentin. Ceramic blocks were cut to 20 blocks with a low-speed diamo
Externí odkaz:
https://doaj.org/article/8491ddbbd4dd418b965010ac6966343b
Autor:
Kusai Baroudi, Giuliane da Cruz Santos, Marina Amaral, Julio Chávez Lozada, Alison Flavio Campos dos Santos, Laís Regiane Silva-Concílio, Larissa Sandy da Silva Leite, João Paulo Mendes Tribst
Publikováno v:
Materials
Materials, Vol 14, Iss 5153, p 5153 (2021)
Materials, 14(18):5153. MDPI AG
Tribst, J P M, Dos Santos, A F C, Santos, G D C, Leite, L S D S, Lozada, J C, Silva-Concílio, L R, Baroudi, K & Amaral, M 2021, ' Effect of cement layer thickness on the immediate and long-term bond strength and residual stress between lithium disilicate glass-ceramic and human dentin ', Materials, vol. 14, no. 18, 5153 . https://doi.org/10.3390/ma14185153
Volume 14
Issue 18
Materials, Vol 14, Iss 5153, p 5153 (2021)
Materials, 14(18):5153. MDPI AG
Tribst, J P M, Dos Santos, A F C, Santos, G D C, Leite, L S D S, Lozada, J C, Silva-Concílio, L R, Baroudi, K & Amaral, M 2021, ' Effect of cement layer thickness on the immediate and long-term bond strength and residual stress between lithium disilicate glass-ceramic and human dentin ', Materials, vol. 14, no. 18, 5153 . https://doi.org/10.3390/ma14185153
Volume 14
Issue 18
This study tested whether three different cement layer thicknesses (60, 120 and 180 μm) would provide the same bonding capacity between adhesively luted lithium disilicate and human dentin. Ceramic blocks were cut to 20 blocks with a low-speed diamo
Publikováno v:
Acta odontologica latinoamericana : AOL. 30(3)
Indirect restorations need to be attached with adhesive luting agents to prevent them from becoming dislodged and provide adequate marginal sealing. The aim of this study was to evaluate bond strength to dentin of self-etching resin cements.75 flat d
Publikováno v:
Acta odontologica latinoamericana : AOL. 27(3)
The aim of this study was to evaluate the film thickness of selfetching resin cement. The following materials were used: Group1, Relyx U100 (3M /ESPE); Group 2, BisCem (Bisco); Group 3, Max Cem (Kerr); Group 4, Set (SDI) and Group 5, Relyx ARC (3M/ES