Soňa Kontárová, Radek Přikryl, Veronika Melčová, Přemysl Menčík, Matyáš Horálek, Silvestr Figalla, Roderik Plavec, Jozef Feranc, Jiří Sadílek, Aneta Pospíšilová
Publikováno v:
Materials, Vol 13, Iss 21, p 4736 (2020)
This paper investigates the effect of plasticizer structure on especially the printability and mechanical and thermal properties of poly(3-hydroxybutyrate)-poly(lactic acid)-plasticizer biodegradable blends. Three plasticizers, acetyl tris(2-ethylhex
Externí odkaz:
https://doaj.org/article/14b311d93b264d84a6c5131ae456c78a
Autor:
Pavel Hutař, Gerald Pinter, Andreas Frank, Jaroslav Kučera, Jan Poduška, Jiří Sadílek, Luboš Náhlík
Publikováno v:
Journal of Mechanical Engineering, Vol 69, Iss 3, Pp 101-106 (2019)
Lifetime of plastic pipes can be estimated by integration of a power law describing the crack kinetics. However, this procedure requires an FEM (finite element method) calculation of the possible crack propagation in the pipe to obtain stress intensi
Autor:
Jiří Sadílek, Pavel Hutař, Jan Poduška, Jaroslav Kučera, Luboš Náhlík, Pavol Dlhý, Andreas Frank
Publikováno v:
Procedia Structural Integrity. 23:293-298
Plastic pipe producers are forced by various initiatives to increase the content of recycled material in their products. The performance of the recycled material is worse than the performance of the virgin material. That is why plastic pipes made ent
Autor:
Matyáš Horálek, Radek Přikryl, Soňa Kontárová, Veronika Melčová, Silvestr Figalla, Přemysl Menčík, Jiří Sadílek, Aneta Pospisilova, Jozef Feranc, Roderik Plavec
Publikováno v:
Materials
Volume 13
Issue 21
Materials, Vol 13, Iss 4736, p 4736 (2020)
Materials . 2020, vol. 13, issue 21, p. 1-27.
Volume 13
Issue 21
Materials, Vol 13, Iss 4736, p 4736 (2020)
Materials . 2020, vol. 13, issue 21, p. 1-27.
This paper investigates the effect of plasticizer structure on especially the printability and mechanical and thermal properties of poly(3-hydroxybutyrate)-poly(lactic acid)-plasticizer biodegradable blends. Three plasticizers, acetyl tris(2-ethylhex
Autor:
Jiří Sadílek, Luboš Náhlík, Jan Poduška, Andreas Frank, Gerald Pinter, Pavel Hutař, Jaroslav Kučera
Publikováno v:
Engineering Fracture Mechanics. 203:18-31
The Cracked Round Bar (abbreviated as CRB in the following) test is used as standardized accelerated testing method for simple ranking of polyethylene pipes based on measuring number of cycles to failure of the cyclically loaded CRB specimen. It can
Autor:
Andreas Frank, Gerald Pinter, Jaroslav Kučera, Pavel Hutař, Jan Poduška, Jiří Sadílek, Luboš Náhlík
Publikováno v:
Solid State Phenomena. 258:174-177
Accelerated tests of the polyethylene pipes are necessary for the pipe lifetime calculations. Accepted methodology for prediction of slow crack grow rate in these materials is fatigue testing of CRB (cracked round bar) specimens. This paper deals wit
Autor:
Gerald Pinter, Andreas Frank, Jiří Sadílek, Jaroslav Kučera, Jan Poduška, Pavel Hutař, Luboš Náhlík
Publikováno v:
Polymer Testing. 54:288-295
This paper deals with residual stress in polyethylene (PE) pipes as an important factor that influences their lifetime. Residual hoop stress distribution in a PE pipe was determined using a methodology previously carried out by the authors on polypro
Autor:
Luboš Náhlík, Martin Ševčík, Jan Poduška, Pavel Hutař, J. Křivánek, Jiří Sadílek, Jaroslav Kučera
Publikováno v:
Polymer Testing. 40:88-98
This paper deals with the experimental determination of residual stress and other inherent properties, density, yield stress, specific enthalpy of fusion and melting point temperature, of a polypropylene grade for pipe applications. The most importan
Autor:
Jiří Sadílek, Jan Poduška, J. Křivánek, Luboš Náhlík, Jaroslav Kučera, Martin Ševčík, Pavel Hutař
Publikováno v:
Key Engineering Materials. 627:141-144
As a result of the production process, there are axial and tangential residual stresses present in pressure pipes made of polymer materials such as polyethylene or polypropylene. The residual stress magnitude and distribution have a significant influ
Publikováno v:
Polymer Testing. 32:106-114
The failure mode termed long time brittle failure (due to slow crack growth – SCG) limits the lifetime of plastic pipes. There are now two main accelerated tests (PENT and FNCT) that enable us to estimate the lifetime of HDPE used in plastics pipes