Autor:
Sudhanshu Mallick, Sarita Zele, Parth Bhatt, Jeroen Oderkerk, Francis Reny Costa, H.P. Sagar, Baloji Adothu, Shashwata Chattopadhyay
Publikováno v:
Solar Energy. 194:581-588
Thermoplastic polyolefin (TPO) is a newly developed non-crosslinking material for photovoltaic (PV) module lamination as an alternative to ethylene–vinyl-acetate (EVA) encapsulant. This article assesses its applicability as an encapsulant material.
Autor:
Sarita Zele, Parth Bhatt, Sudhanshu Mallick, Baloji Adothu, Purnendu Kartikay, Francis Reny Costa, Jeroen Oderkerk
Publikováno v:
Web of Science
Thermoplastic polyolefin (TPO) is a newly developed non-crosslinking encapsulant for the crystalline silicon PV modules lamination. The degree of crystallinity and thermal stability of TPO have been studied and compared with the most commonly used et
Autor:
Baloji Adothu, Jeroen Oderkerk, Sarita Zele, Parth Bhatt, Francis Reny Costa, Sudhanshu Mallick
Publikováno v:
Materials Chemistry and Physics. 243:122660
Ethylene-vinyl acetate (EVA) is the predominating material of choice for making the encapsulant film for photovoltaic (PV) modules. The easy accessibility, low cost, high transparency, long track record, widespread know-how on processability and perf
Autor:
Jeroen Oderkerk, Torbjörn Reitberger, Francis Reny Costa, Thomas Hjertberg, V. Englund, Ulf W. Gedde, Wenbin Yu
Publikováno v:
Polymer Degradation and Stability. 111:1-6
A series of polyethylene tape samples containing 8 different phenolic antioxidants (concentration = 0.1 ± 0.01 wt.%) were exposed to water containing 10 ppm chlorine dioxide buffered to pH = 6.8 at 70 °C for different periods of time. The degradati
Autor:
Thomas Hjertberg, Francis Reny Costa, Jeroen Oderkerk, Torbjörn Reitberger, Ulf W. Gedde, Wenbin Yu
Publikováno v:
Polymer Degradation and Stability. 97:2370-2377
This thesis presents a study of antioxidant depletion in water containing chlorinated species (water containing 10 ppm either Cl2 or ClO2, buffered to pH = 6.8), the degradation products in the aqueous phase, and polyethylene pipe degradation scenari
Autor:
Jeroen Oderkerk, Gabriël Groeninckx
Publikováno v:
Polymer. 43:2219-2228
Binary nylon6/rubber blends with 50 or 60 weight percent of an EPDM rubber exhibit co-continuous morphologies and thereby relatively poor mechanical properties. This paper describes methods to develop nylon6/EPDM blends with a high amount of finely d