Publikováno v:
Welding in the World. 66:2171-2190
Autor:
J. C. Lippold, R. A. Wheeling
Publikováno v:
Journal of Failure Analysis and Prevention. 17:796-801
The nature of cracking during continuous casting of steel strip was investigated. Samples removed from steel strip for fractographic analysis were heavily oxidized, preventing effective evaluation of the fracture surface. In order to remove the oxida
Autor:
J. C. Lippold, Thomas J. Lienert
Publikováno v:
Science and Technology of Welding and Joining. 8:1-9
Pulsed Nd:YAG laser welds were produced on 23 different austenitic stainless steel alloys of known composition. The primary solidification mode (PSM) and solidification cracking susceptibility of individual welds on each alloy were identified and cor
Autor:
J. C. Lippold
Publikováno v:
Journal of Materials Science. 30:4155-4160
The post-weld ageing behaviour of two commercial aluminium-lithium alloys, 2090 and 8090, was evaluated. Both a 2319 and 5556 filler material were used for preparing welds in Alloy 2090, while only the 5556 filler material was used with Alloy 8090. W
Autor:
J C Lippold, G S Frankel
Stainless steel components are often joined by welding when fabricated into structures. Fusion welding of these steels results in the formation of carcinogenic Cr(VI) in the weld fumes as a result of the Cr content of the commonly used filler metals.
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::3d233017f670acae8c18dc6647cf4df5
https://doi.org/10.21236/ada520640
https://doi.org/10.21236/ada520640
Failure of welded components can occur during service as well as during fabrication. Most common, analyses of the resistance of welded components against failure are targeted at crack avoidance. Such evaluations are increasingly carried out by modern
Publikováno v:
Metallurgical Transactions A. 19:35-50
The heat-affected zone (HAZ) hot-cracking behavior of Alloy 800 was investigated with hot ductility (Gleeble) testing during a simulated HAZ thermal cycle. Microstructural analyses were performed by optical metallography, fractography, electron micro
Publikováno v:
Metallurgical Transactions A. 16:1835-1848
Multipass weld deposits produced with a Mn-modified Type 316L filler material exhibited fracture toughness nearly 100 MPa√m less than that of a conventional 316L filler material when tested at 4.2 K. Although fracture in both materials occurred by
Publikováno v:
Journal of Materials Science Letters. 7:1204-1208
Etude de la fissuration des superalliages (Incoloy 905 et 903) par microscopie electronique a balayage et par microscopie optique apres soudage a l'arc
Publikováno v:
Holm, H, Bach, H, Hansen, M V & Franke, D 2003, Planning of Finite Element Modelled Welding Control Variable Trajectories by PI-Controllers and by Iterative Learning . in S A D T D J C L H B S J M Vitek (ed.), Trends in Welding Research, Proceedings of the 6th International Conference . ASM International, pp. 967-972, Trends in Welding Research, Pine Mountain, Georgia, United States, 15/04/2002 .
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=dedup_wf_001::1f9848d2e7d8625017fc80623a96db8c
https://vbn.aau.dk/da/publications/8b000fa0-9c2d-11db-8ed6-000ea68e967b
https://vbn.aau.dk/da/publications/8b000fa0-9c2d-11db-8ed6-000ea68e967b