Polymer Degradation and Stability. 188:109575
Photooxidation of polypropylene (PP) was investigated by chemiluminescence (CL) after UV irradiation of main wavelengths of 254 nm and 365 nm in air at an ambient temperature. From the kinetic analysis of CL intensity change just after irradiation, C
Publikováno v:
Key Engineering Materials. 352:259-262
Autor:
Takuro Nakashima, Yoshitomo Masuda, Michihiro Asakawa, Reiji Hattori, Ryo Sakurai, Norio Nihei, Itsuo Tanuma, Yokoo Akihiko
Publikováno v:
SID Symposium Digest of Technical Papers. 38:1462-1465
The thin and flexible LSI driver with a thickness of less than 40μm for passive-matrix driven Quick-Response Liquid Powder Display (QR-LPD™) was successfully mounted onto the flexible printed circuit (FPC). The mounted LSI on the plastic substrate
Novel Type of Bistable Reflective Display (QR-LPD®) and Material Design of Electronic Liquid Powder®
Publikováno v:
NIP & Digital Fabrication Conference. 23:624-627
Publikováno v:
Journal of the Japan Society of Colour Material. 80:253-257
Publikováno v:
The Journal of the Institute of Image Information and Television Engineers. 59:1266-1269
Publikováno v:
Seikei-Kakou. 7:499-504
Publikováno v:
SAE Technical Paper Series.
Several kinds of polymers for liquid crystal/polymer complex film (LC/P film) and their modifications had been examined in order to improve their thermal stabilities and mechanical durabilities. Crosslinked rubbery resin; modified poly butadiene, was
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::79fe183c4c714a5eb31a4aa35daab420
https://doi.org/10.1016/b978-1-4832-8380-7.50084-5
https://doi.org/10.1016/b978-1-4832-8380-7.50084-5