Publikováno v:
Journal of Welding and Joining. 40:33-39
The demand for liquefied-natural-gas-fueled tanks on ships is growing in accordance with IMO 2020 regulations. The use of high manganese steel has increased recently, as this material can be applied at cryogenic service temperatures according to IGF
Publikováno v:
Applied Sciences, Vol 10, Iss 8613, p 8613 (2020)
Applied Sciences
Volume 10
Issue 23
Applied Sciences
Volume 10
Issue 23
Unstable fractures generally occur in brittle materials under low-temperature service conditions. Toughness and welding residual stress are the main factors that should be evaluated when defining a brittle crack propagation path. In this study, a rai
Publikováno v:
International Journal of Offshore and Polar Engineering. 27:260-265
Publikováno v:
Materials Chemistry and Physics. 184:118-129
The effect of the alloying elements, the carbon, nickel, and the titanium in particular, on the hot ductility behavior of high manganese steel for cryogenic applications was investigated. A hot ductility test was carried out to clarify the mechanism
Publikováno v:
Journal of Non-Crystalline Solids. 432:218-226
The effect of TiO 2 /SiO 2 and SiO 2 /Al 2 O 3 ratio on the wettability of the TiO 2 –MnO–SiO 2 –Al 2 O 3 quaternary welding flux system was studied using the sessile drop method by measuring the contact angle at the liquid/solid interface. The
Publikováno v:
Theoretical and Applied Fracture Mechanics. 109:102747
Residual stress variations were determined through small- and large-scale specimen welds using neutron diffraction to evaluate the effect of residual stress on the brittle crack propagation path. The results revealed that significant tensile stresses
Publikováno v:
Materials Science and Engineering: A. 618:295-304
In the present study, the hot ductility behavior and hot cracking susceptibility of high manganese cast steel were investigated. Based on the 18Mn–0.6C alloy, a nickel was added for cryogenic impact toughness by maintaining the low temperature aust
Publikováno v:
Metallurgical and Materials Transactions A. 45:2046-2054
Oxide inclusions in high-Mn steel welds were analyzed and almost all of which were found to belong to the MnO-Al2O3-SiO2 system. In this study, the inclusions were categorized based on MnS morphology into the following two types: (1) aluminosilicate
Publikováno v:
Metals and Materials International. 16:489-494
Various fluorides, CaF2, Na3AlF6, K2SiF6, MnF3, and MgF2, were added to rutile-type flux cored wires at concentrations of 1.8–2.3% and their effects on hydrogen reduction in weld metals were studied. All the fluorides reduced the hydrogen content b
Autor:
Soon Taik Hong, Il Wook Han
Publikováno v:
Journal of the Korean Welding and Joining Society. 28:5-12
Design temperature(℃) Steels-273 ~ -196 Stainless steel-196 ~ -10 Al killed steel, Fe-Ni steel-10 ~ 350Plain carbon steel, Si-Mn steel, Mn-Mo-Ni steel350 ~ 450Fine grained steel, Mn-Mo steel, Mn-Mo-Ni steel450 ~ 500 C-Mo steel, 2.25Cr-1Mo steel500