Publikováno v:
Glass Physics and Chemistry. 42:547-553
The characteristics (composition of the quenched samples, ingot, and evaporation products) are studied of the melt of the corium–high alumina cement system in a weight ratio of 1: 1. In the quenched samples of the melt and ingot, signs of phase sep
Publikováno v:
Glass Physics and Chemistry. 42:484-489
The behavior of a melt of a UO2–ZrO2–SiO2–Fe3O4–CaO–Al2O3 system that is formed in the case of the dilution of corium (a melt of a UO2–ZrO2–Zr system) with sacrificial materials (a mixture of aluminum and iron oxides with Portland cemen
Publikováno v:
Glass Physics and Chemistry. 42:270-276
Changes in the intensity of evaporation and the composition of condensing oxides are experimentally studied upon diluting corium by iron(III) oxide and Portland cement. It is found that the formation rate of aerosols over the melt is reduced upon dil
Publikováno v:
Inorganic Materials. 47:1579-1583
A contactless method of electrical resistivity measurement for high-temperature melts is described. The method is based on induction melting in split water-cooled crucible and solving the inverse problem of electromagnetic field with the use of the t
Autor:
N. V. Gus’kova, B. A. Lavrov, Yu. P. Udalov, A. S. Sidorov, I. V. Poznyak, A. Yu. Pechenkov, M. N. Mikhailov
Publikováno v:
Glass Physics and Chemistry. 37:85-97
The process of formation of the skull on the St-3 steel in contact with molten ferroalloys and multicomponent oxides at temperatures of 1600 and 2000°C, respectively, has been investigated. The data obtained have been compared with the results on th
Publikováno v:
Glass Physics and Chemistry. 34:623-633
The morphology of the quenched and slowly crystallized samples in the ZrO2-Al2O3 system is investigated in the composition range 25–70 wt % ZrO2. It is revealed that, irrespective of the cooling rate, the samples contain large baddeleyite (or corun
Publikováno v:
Glass Physics and Chemistry. 32:479-485
The morphology of the crystalline phases prepared at different cooling rates, temperatures, and compositions of melts in the ZrO2-Al2O3 system is investigated. It is established that both the quenched and slowly crystallized samples containing 35–7