Metals, Vol 7, Iss 1, p 29 (2017)
The corrosion of Ti-54M titanium alloy processed by hot rotary swaging and post-annealed to yield different grain sizes, in 2 M HCl solutions is reported. Two annealing temperatures of 800 °C and 940 °C, followed by air cooling and furnace cooling
Externí odkaz:
https://doaj.org/article/19a7a48bbce748a9872f2da447e3b357
Publikováno v:
Journal of Materials Engineering and Performance. 24:2074-2084
TIMETAL 54M is a newly developed (α + β) titanium alloy with nominal composition Ti-5Al-4V-0.6Mo-0.4Fe. The alloy can provide a cost benefit over Ti-6Al-4V due to improved machinability and formability. In the present work, evolution of mechanical
Publikováno v:
Metals, Vol 7, Iss 1, p 29 (2017)
Metals; Volume 7; Issue 1; Pages: 29
Metals; Volume 7; Issue 1; Pages: 29
The corrosion of Ti-54M titanium alloy processed by hot rotary swaging and post-annealed to yield different grain sizes, in 2 M HCl solutions is reported. Two annealing temperatures of 800 °C and 940 °C, followed by air cooling and furnace cooling
Publikováno v:
Advances in Materials Science and Engineering, Vol 2015 (2015)
Fully reversed bending fatigue tests were performed on polished hour-glass specimens of commercially pure titanium grade 1 with three different grain sizes, that were produced by severe plastic deformation (rotary swaging) and subheat treatments, in
Autor:
Hasan Al-Khazraji, Mansour Mhaede, N. Schell, Heinz Günter Brokmeier, Z.Y. Zhong, M.Z. Salih, Lothar Wagner
Publikováno v:
Metallurgical and Materials Transactions B. 45:1579-1579
Cold rolling (CR) leads to a heavy changes in the crystallographic texture and microstructure, especially crystal defects, such as dislocations, and stacking faults increase. The microstructure evolution in commercially pure titanium (cp-Ti) deformed
Autor:
Sherif, El-Sayed M., El Danaf, Ehab A., Abdo, Hany S., El Abedin, Sherif Zein, Al-Khazraji, Hasan
Publikováno v:
Metals (2075-4701); Jan2017, Vol. 7 Issue 1, p29, 13p
Publikováno v:
Journal of Materials Engineering & Performance; May2015, Vol. 24 Issue 5, p2074-2084, 11p
Autor:
Alkhazraji, Hasan, Salih, Mohammed, Zhong, Zhengye, Mhaede, Mansour, Brokmeier, Heinz-Günter, Wagner, Lothar, Schell, N.
Publikováno v:
Metallurgical & Materials Transactions. Part B; Aug2014, Vol. 45B Issue 4, p1579-1579, 1p
Autor:
ALkhazraji, Hasan, Salih, Mohammed, Zhong, Zhengye, Mhaede, Mansour, Brokmeier, Hans-Günter, Wagner, Lothar, Schell, N.
Publikováno v:
Metallurgical & Materials Transactions. Part B; Aug2014, Vol. 45B Issue 4, p1557-1564, 8p
Autor:
Keall, Edward J.
Publikováno v:
World Archaeology; Feb1983, Vol. 14 Issue 3, p378-392, 15p