Test specimens of stainless steel DIN 1.4948, which is similar to AISI Type 304, have been irradiated at 723 and 823 K up to fluences of 1 X 10 2 3 neutrons (n).m - 2 and 5 X 10 2 4 n.m - 2 (E > 0.1 MeV). These are representative conditions for the r
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::708de97dac542be86a0763e4c808563b
https://doi.org/10.1520/stp38183s
https://doi.org/10.1520/stp38183s
Publikováno v:
Engineering Fracture Mechanics. 11:275-283
Crack growth rate and crack closure during fatigue of type 304 stainless steel are measured with an optical microscope and television camera. Based on the crack closure data an effective stress intensity range ΔK eff is calculated. The da / dn vs Δ
Autor:
A.R. Korko, D. Perry, H.U. Staal, J.F.W. Markgraf, G. Dassel, J. Bordo, G. Snijders, K.W. de Haan
Publikováno v:
NDT International. 22:242
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Conference
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.