Zobrazeno 1 - 10
of 18
pro vyhledávání: '"H. D. Solomon"'
Autor:
H. D. Solomon, E. D. Tolksdorf
Publikováno v:
Journal of Electronic Packaging. 118:67-71
Autor:
H. D. Solomon
Publikováno v:
Journal of Electronic Packaging. 115:173-179
This study employed different cycle frequencies, to determine the influence of cycle frequency on the fatigue life of leaded chip carrier printed wiring board (LCC/PWB) interconnections. Real LCC/PWB interconnections were mechanically cycled at 35°C
Autor:
H. D. Solomon
Publikováno v:
Journal of Electronic Packaging. 113:102-108
This paper describes the 35°C and 150°C low cycle fatigue behavior of Sn96 solder (96.5 Sn/3.5 AG), the tin silver eutectic. There is a considerable amount of anecdotal information which says that this solder is superior to eutectic solder in its f
Autor:
H. D. Solomon
Publikováno v:
Journal of Electronic Packaging. 113:186-190
Publikováno v:
JOM. 42:7-11
Despite the serious impact of stress-corrosion cracking and corrosion fatigue, the relevant design and operational guidelines for light-water nuclear reactors are often just rules of thumb which identify susceptibility or codes which only quantify th
Autor:
H. D. Solomon
Publikováno v:
Journal of Electronic Packaging. 112:123-128
This paper describes the fatigue behavior of a Pb rich solder, 92.5Pb, 2.5Ag, 5.0Sn (Indalloy 151), tested at −50°C and +150°C. The results are compared to previously reported studies of 60Sn/40Pb solder and to tests of Indalloy 151 performed at
Autor:
C. Amzallag, H. D. Solomon
Publikováno v:
Volume 1: Codes and Standards.
This paper compares the various models used to describe the fatigue behavior of Austenitic Stainless Steels. This was done for newly produced GE/EDF fatigue results and for hundreds of other data points gleaned from the literature. This comparison wa
Autor:
H. D. Solomon
Publikováno v:
Journal of Electronic Packaging. 111:75-82
This paper describes low cycle fatigue test run at −50°C, 35°C, 125°C, and 150°C on thin 60 Sn/40 Pb solder joints, tested in simple shear. The low cycle fatigue behavior was found to be a function of the criteria used to define the fatigue lif
Autor:
H. D. Solomon
Publikováno v:
CORROSION. 41:512-517
This paper addresses the question of the combined effect of carbon content and prior cold work on the sensitization of AISI 304 stainless steel (SS). It was found that prior.cold work increased the critical cooling rate required to produce sensitizat
Autor:
H. D. Solomon
Publikováno v:
Nuclear Technology. 29:86-93
The high strain crack growth rate in isotropic Zircaloy-2 welds was measured using strain cycling with controlled limits of plastic strain. The crack growth rate was found to be a function of the longitudinal plastic strain range or the longitudinal