Mohammed A. Sanhoob, Emad N. Shafei, Abuzar Khan, Galal A. Nasser, Idris Bakare, Oki Muraza, Mohammed Z. Al-Bahar, Ali N. Al-Jishi, Hameed H. Al-Badairy, Aniz C. Ummer
Publikováno v:
ACS Omega, Vol 7, Iss 12, Pp 10317-10329 (2022)
Externí odkaz:
https://doaj.org/article/947845258cfb475dbe629a949feee02b
Autor:
Al-Shafei, Emad N., Robert Brown, D., Katikaneni, Sai P., Aljama, Hassan, H. Al-Badairy, Hameed
Publikováno v:
In Chemical Engineering Journal 1 September 2021 419
Publikováno v:
Protective Systems for High Temperature Applications EFC 57 ISBN: 9781003421498
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::464a3ba15588dbb17bc3aff18fa2e414
https://doi.org/10.1201/9781003421498-9
https://doi.org/10.1201/9781003421498-9
Autor:
Mohammed A, Sanhoob, Emad N, Shafei, Abuzar, Khan, Galal A, Nasser, Idris, Bakare, Oki, Muraza, Mohammed Z, Al-Bahar, Ali N, Al-Jishi, Hameed H, Al-Badairy, Aniz C, Ummer
Publikováno v:
ACS omega. 7(12)
This study emphasizes tuning the synthesis conditions of MFI zeolites to achieve better catalytic properties by optimizing the mesoporosity, the balance between Brønsted and Lewis sites, and the zeolite particle sizes. The MFI zeolites were hydrothe
Autor:
Yassine Slimani, R. A. Al-Mohsin, Munirah Abdullah Almessiere, H. Al-badairy, F. Ben Azzouz, Amal L. Al-Otaibi
Publikováno v:
Journal of Low Temperature Physics. 192:100-116
Here we compare the microstructure and flux pinning properties of polycrystalline YBa2Cu3O7-d (Y-123 or YBCO) containing either Al2O3 or Zn0.95Mn0.05O nanoparticles. Samples were prepared using a standard solid-state reaction process, and nanoparticl
Publikováno v:
Materials and Corrosion. 59:414-422
During the oxidation, in laboratory air, of thin foils of Fe-20Cr-5Al based alloys, voids were formed in the substrate beneath the outer protective alumina scale after times varying from 50 h at 900 °C to 10 min at 1200 °C. Once the substrate alumi
Publikováno v:
Materials Science and Technology. 22:1316-1324
A scanning electron microscope (SEM) study was conducted of α alumina scales developed on the surface of FeCrAl alloys during high temperature oxidation, using backscattered electron imaging, cathodoluminescence (CL) imaging, electron backscatter di
Publikováno v:
Materials and Corrosion. 56:848-853
In the present work the effects of single or combined minor additions of Zr, Hf, Ti and C on the oxidation behaviour of Y-containing, FeCrAl alloys have been studied. For this purpose high-purity, model alloys with single or multiple minor alloying a
Publikováno v:
Materials and Corrosion. 56:867-873
The degradation of a variety of alumina-forming Fe20Cr5Al based alloys has been investigated at temperatures ranging from 1100°C to 1300°C for up to 4000 h (100 h/cycle) in different oxidising environments such as laboratory air, air + 10 vol% H2O,
Publikováno v:
Scopus-Elsevier
The chemical failure of commercial FeCrAlRE (where RE is a reactive element) alloys, such as Aluchrom YHf and Kanthal AF foils (30–50 μm thick), is induced by oxidation, in air, at 800–950°C. This is also the life limiting process of this famil