Publikováno v:
Wear. 267:1415-1419
The effect of boron on the abrasive wear behavior of the austenitic Fe–Cr–C–Si–B hardfacing alloys was investigated with varying boron concentration. It was found that the abrasive wear resistance of the hardfacing alloys increased up to 50%
The effects of Mn and B on the cavitation erosion resistance of austenitic Fe-base hardfacing alloys
Publikováno v:
Materials Science and Engineering: A. 477:204-207
The effects of manganese and boron on the cavitation erosion behavior of austenitic Fe–Cr–C–Si– x Mn– y B ( x = 0, 10 wt%, y = 0, 0.3 wt%) hardfacing alloys were investigated by using a vibratory cavitation erosion tester. It was found that
Publikováno v:
Journal of Alloys and Compounds. 449:184-187
For the surface modification of polymer, wet-chemical pretreatments using a strong acid such as chromic, sulfuric and potassium-permanganate acid have been performed. However, these methods tend to have inherent problems of uniformity, reproducibilit
Autor:
Joung Ah Kang, Seon Jin Kim, Sun Doo Kim, Ji Hui Kim, Gyung Guk Kim, Kyung Jong Lee, Kwon Yeong Lee, Chong Seung Yoon
Publikováno v:
Solid State Phenomena. :1477-1480
Hydrogen redistribution caused by thermotransport in the Zr-1.0Nb-1.0Sn-0.1Fe alloy under the temperature gradient which is likely to be encountered between nuclear fuel cladding and primary cooling water (300-340) was investigated. The heat of trans
Publikováno v:
Catalysis Communications. 8:861-864
In the present study, the pretreatment of glass-epoxy resin using photoreaction of TiO 2 sol prepared by hydrothermal method was investigated. The surface properties for the pretreated substrate were examined, and the change of contact angle was meas
Publikováno v:
Materials Science Forum. :75-78
The pretreatment of ABS (acrylonitrile-butadiene-styrene) plastics prior to metallization has been generally performed with strong acids, such as sulfuric, chromic, or potassium-permanganate acid. However, conventional wet-chemical pretreatment prese
Publikováno v:
Wear. 262:845-849
In this study, sliding wear behavior of newly developed Fe-base Co-free hardfacing alloy (Fe–Cr–C–Si) was investigated and compared to that of Stellite 6 and Fe-base NOREM 02 in the temperatures ranging from 300 to 575 K under a contact stress
Publikováno v:
Surface and Coatings Technology. 201:3761-3766
The wet-chemical preconditioning process of polymers prior to metallization is generally performed with a strong acid bath such as a chromic, sulfuric or potassium- permanganate solution. Although the method is widely used in industrial applications,
Publikováno v:
Tribology Letters. 26:131-135
The effects of temperature and sliding distance on the metal-to-metal wear behavior of austenitic Fe-20Cr-1.7C-1Si hardfacing alloy were investigated in air in the temperature range from 25 to 450 °C. The applied contact stress was 55 MPa and the ma
Publikováno v:
Journal of Nuclear Materials. 352:85-89
The cavitation erosion behavior of Fe–Cr–C–Si–xMn (x = 5, 10 and 15 wt%) alloys were investigated for 50 h using 20 kHz vibratory cavitation erosion test equipment. Low-Mn alloys ( 10 wt% Mn) exhibited the γ → α′ and γ → e strain-ind