Roger Courchinoux, Stéphane Bouillet, Thierry Donval, Christel Ameil, Laurent Lamaignère, Odile Bonville, Sandrine Fréville, Romain Parreault, Jérôme Daurios, Nadja Roquin, Sébastien Martin, Gerard Raze, Isabelle Lebeaux, Gael Gaborit, Vincent Beau, Sandy Cavaro, Christophe Leymarie, Laure Eupherte
Publikováno v:
Journal of the Optical Society of America. A, Optics, image science, and vision. 36(11)
The Laser MegaJoule (LMJ) is a high-power laser dedicated to laser-plasma experiments. At the beginning of the project in the mid-1990s, an optical metrology laboratory was created at CEA to help accomplish all the steps in the construction of this l
Autor:
Hervé Mathis, X. Leborgne, D. Damiani, Marc Loiseau, C. Maunier, Thierry Donval, G. Duchateau, Gerard Raze, Gael Gaborit, Laurent Lamaignère, B. Bertussi, A. . Dyan
Publikováno v:
SPIE Proceedings.
In this paper, we present various laser conditioning experiments which have been performed with KDP SHG and DKDP THG samples. The different conditioning facilities used delivered laser pulses at 351 nm in the nanosecond (from 3 to 12 ns) or in the su
Autor:
Jérôme Néauport, Laurent Lamaignère, Gerard Raze, Annelise During, Herve Bercegol, Hervé Piombini, Philippe Bouchut
Publikováno v:
High-Power Laser Ablation V.
For high power laser applications like the "Laser Megajoule" facility under construction in France, laser-induced damage threshold (LIDT) in fused silica is a limitation. CEA has made efforts to improve LIDT at the wavelength of 351 nm. Polishing and
Autor:
Thierry Donval, Herve Bercegol, A. Boscheron, Laurent Lamaignère, E. Mazataud, Caroline Sudre, Marc Loiseau, Gerard Raze, C. Lepage
Publikováno v:
SPIE Proceedings.
Variable experimental conditions were used to measure the occurrence of front surface, rear surface and filamentation damage in synthetic fused silica windows. Experiments were performed at 355 nm with a table-top beam of mm-size, and at 351 nm with
Autor:
Caroline Sudre, A. Boscheron, Michel A. Josse, Edouard Bordenave, Roger Courchinoux, Thierry Donval, Herve Bercegol, Laurent Lamaignère, E. Mazataud, C. Lepage, Marc Loiseau, Gerard Raze
Publikováno v:
SPIE Proceedings.
Experiments have been performed to measure the rate of laser-induced damage growth at the rear surface of fused silica windows at 1064, 1053 and 351 nm. One test bench delivered 9 ns monomode gaussian pulses at 10 Hz and 1064 nm. The size of the focu
Publikováno v:
SPIE Proceedings.
The purpose of this paper is to gather experimental elements allowing for the prediction of laser damage on full size components installed on high power Nd-glass laser lines. Damage can initiated on material defects, which aren’t known in their nat
Autor:
Caroline Sudre, Laurent Lamaignère, Thierry Donval, Herve Bercegol, Roger Courchinoux, Gerard Raze, Michel A. Josse, Marc Loiseau
Publikováno v:
SPIE Proceedings.
The functional lifetime of large aperture optical components used in high power lasers, like LIL and LMJ facilities, is mainly determined by laser damage measurements. We present experimental procedures and statistical analysis, made on small samples
Autor:
Gerard Raze, Michel A. Josse, Thierry Donval, Marc Loiseau, Roger Courchinoux, Caroline Sudre, Herve Bercegol, Laurent Lamaignère
Publikováno v:
SPIE Proceedings.
The functional lifetime of large aperture components used in high power lasers, like LIL and LMJ facilities, is mainly determined by laser damage measurements. Automatic damage test benches allow to obtain more data in less time than traditional test
Publikováno v:
Laser-Induced Damage in Optical Materials: 2002 and 7th International Workshop on Laser Beam and Optics Characterization.
Samples of Neodymium doped laser glass were irradiated by the 1ω beam of a Nd:glass laser that delivers up to 80 J during a 3-ns pulse duration. Prior to this experiment, platinum inclusions were revealed by a systematic scanning with a lab-scale Nd
Autor:
Jean-Marie Morchain, Laurent Lamaignère, Herve Bercegol, Michel A. Josse, Marc Loiseau, Gerard Raze
Publikováno v:
Laser-Induced Damage in Optical Materials: 2002 and 7th International Workshop on Laser Beam and Optics Characterization.
The growth of damage sites on the rear surface of fused silica plates was studied as a function of fluence and angle of incidence. At 1053 nm, a 70 J beam, 3 ns in pulselength, was directed to a 5 cm 2 zone on a bare fused silica window. Initiation a