Zobrazeno 1 - 10
of 55
pro vyhledávání: '"G.L.P. Berning"'
Publikováno v:
Applied Surface Science. 157:129-134
A total of 3000 A Tb followed by 200 A Si (to reduce oxidation of Tb during annealing) was deposited onto SiO2. The samples were annealed at 500°C from 7 to 97 min in HV. Rutherford backscattering (RBS) studies were performed on the annealed Tb on S
Publikováno v:
Materials Chemistry and Physics. 58:26-30
Samples of Tb and Dy as well as their silicides were oxidized in high vacuum under controlled conditions for oxygen exposures ranging up to 50 L (1 L = 1 × 10 −6 Torr·s). The oxides were studied by Auger electron spectroscopy (AES) and ion scatte
Publikováno v:
Applied Surface Science. 140:63-69
Auger electron spectroscopy (AES) and cathodoluminescence (CL) measurements showed that surface reactions with the consequent loss of CL intensity occur for both the ZnS:Cu,Al,Au and ZnS:Ag,Cl phosphor powders during prolonged electron bombardment. A
Autor:
H.C. Swart, G.L.P. Berning
Publikováno v:
Surface and Interface Analysis. 26:420-424
A 2000 A layer of Tb followed by a 200 A layer of Si was deposited onto an SiO2 substrate. The samples were annealed from 480°C for 4 min to 800°C for 120 min in a high vacuum (p⩽2×10−7 Torr). It was inferred from Auger depth profiles and peak
Publikováno v:
Surface and Interface Analysis. 26:337-342
The phosphor powder ZnS:Cu,Al,Au has been investigated extensively as a possible green phosphor for field emission displays (FEDs). Phosphor powders of ZnS:Cu,Al,Au have been subjected to electron bombardment (1–5 keV) at oxygen pressures ranging f
Publikováno v:
Applied Surface Science. 120:9-14
ZnS:Cu,Al,Au phosphor powder has been subjected to 2 keV electron bombardment at an oxygen pressure of 1×10−6 Torr. Auger electron spectroscopy (AES) and cathodoluminescence (CL), both excited by the same electron beam were used to monitor changes
Autor:
G.L.P. Berning, H.C. Swart
Publikováno v:
Materials Chemistry and Physics. 41:251-256
Austenitic Fe-26Mn-7Al-0.9C was annealed for 1 h at atmospheric pressure at 200, 400, 600 and 800 °C. Low-energy Auger transitions and detail X-ray photoelectron spectra were used to characterize the oxide layers formed on the alloy during annealing
Autor:
G.L.P. Berning, H.C. Swart
Publikováno v:
Applied Surface Science. 78:339-343
Pure Tb as well as TbSi 1.7 /Si(100) were oxidized at 600°C for 30 min at atmospheric pressure. Auger, XPS and XRD spectra of the samples were measured before and after oxidation. The XRD results show that pure Tb oxidizes to form TbO 1.81 while the
Autor:
H.C. Swart, G.L.P. Berning
Publikováno v:
Applied Surface Science. 78:77-82
By evaporating Fe onto Si(100) substrates in an oxygen ambient, oxygen concentrations of 2, 3, 10 and 35 at% could be gettered in four Fe films. Auger electron spectroscopy (AES) and X-ray photoelectron spectroscopy (XPS) were used to investigate the
Autor:
H.C. Swart, G.L.P. Berning
Publikováno v:
Applied Surface Science. 73:260-263
The effect of different (0.5 to 4 keV) Ar + energy ions on the composition of the surfaces of TbSi 1.7 and FeSi has been monitored by Auger electron spectroscopy. During Ar + ion bombardment of TbSi 1.7 the surface was enriched with Si while the FeSi