Publikováno v:
Metal Science and Heat Treatment. 50:73-76
The structure, hardness, phase composition, and wear intensity of the nitrided layer on steel 12Kh18N10T formed in a medium of nitrogen at a pressure of 160 MPa at a temperature of 1150°C with a hold of 3 h are studied.
Publikováno v:
Metal Science and Heat Treatment. 46:227-229
The structure, hardness, and thickness of the hardened layer on steel 16Kh2N3MFBAYu-Sh (martensitic class), steel 12Kh18N10T (austenitic class), and iron are studied after nitriding at a nitrogen pressure of 100 – 150 MPa and temperature of 950 –
Autor:
G. G. Mukhin, M. S. Pavlov
Publikováno v:
Metal Science and Heat Treatment. 36:313-317
Carbides are necessary component part of the structure in high-speed steels. The wear resistance, heat resistance, and strength of these steels markedly depend on the amount of carbides, the ratio between different types of carbides, and their states
Publikováno v:
Metal Science and Heat Treatment. 44:435-436
Autor:
M. S. Pavlov, G. G. Mukhin
Publikováno v:
Metal Science and Heat Treatment. 40:394-395
Nitriding of cutting tools is used to improve their endurance. The small thickness of the nitrided layers does not make it possible to evaluate their heat resistance by the standard method. This has made it necessary to develop a method for independe
Publikováno v:
Metal Science and Heat Treatment. 28:840-843
1. Rapid quenching causes supersaturation of the matrix with alloying elements, an abrupt refinement of the second phases, and even amorphization of the matrix of alloys type Fe−Mo (Cr, V)−B(C); this increases their hardness and strength, and at
Publikováno v:
Journal of Non-Crystalline Solids. 103:45-48
Changes of mechanical properties of rapidly quenched Fe-Mo-B alloys have investigated versus cooling rate (10 2 –10 6 °C/s), alloying elements content (Cr, V, C) and heat treatment cycles at 550–650 °C (up to 20 h).
Publikováno v:
Metal Science and Heat Treatment. 30:903-907
1. Increased silicon and boron content of amorphous alloys with 15–30% (B+Si) causes a rise of the crystallization temperature, and consequently, greater stability of the metastable state. 2. The principal phase in the crystallization of amorphous
Autor:
G. G. Mukhin, Yu. V. Efimo
Publikováno v:
Journal of Materials Science Letters. 4:908-911
Autor:
G. G. Mukhin, L. P. Korotkova
Publikováno v:
Metal Science and Heat Treatment. 30:269-272
1. In annealing of sprayed high-speed steels the dispersion of the structural constituents, including the carbides, is maintained. 2. The carbide content in the sprayed powders increases after annealing, M23C6 carbide is formed, the content of M2C ca