Zobrazeno 1 - 10
of 41
pro vyhledávání: '"Fumihiro Suzumura"'
Autor:
Chiharu Fukushima, Gonojo Katayama, Fumihiro Suzumura, Masahiro Ikeda, Hiromasa Makihara, Kozo Ohtani
Publikováno v:
Advanced Materials Research. :4064-4067
The purpose of this paper is to estimate thermal deformation of machine tool model by using transfer function with time delay. The prediction method of thermal deformation based on frequency domain is constructed from transfer function between specif
Autor:
Fumihiro Suzumura, Akihiro Iwamura
Publikováno v:
The Proceedings of Conference of Chugoku-Shikoku Branch. :1009
Publikováno v:
Modern Physics Letters B. 22:839-844
AE was measured under a static tensile load for the thermally sprayed ceramic coating in order to investigate the relationship between the detected m-value and the destruction (delamination) of the sprayed coating. This was an effective method to det
Publikováno v:
Materials Science Forum. :2687-2692
Fe 3 O 4 and Mo and were added to hot-press sintered Si 3 N 4 ceramics to improve their lipophilic and mechanical properties. The bending strength, relative density, hardness and fracture toughness of Si 3 N 4 ceramics with addition of Fe 3 O 4 and M
Publikováno v:
Journal of the Japan Institute of Metals. 71:330-335
Recently, the use of Pb-free solder has caused early deterioration and decreased lifetime of the soldering iron tip. Therefore, it is critical to find a solution to this problem. In this study, the changes in the properties of a ceramics/metal compos
Publikováno v:
Key Engineering Materials. :999-1002
Detection of delamination of a thermally sprayed coating on an SUS304 substrate was carried out nondestructively using electronic speckle pattern interferometry (ESPI) method in both static and cyclic tests at T=298 K and 873 K. Results showed that t
Publikováno v:
Journal of the Japan Institute of Metals. 70:962-967
Wettability of a material surface plays a very important role in solid-liquid interaction phenomena used to analyze material surface treatments, soldering, and for the improvement of material properties with surfactant solutions and lubricants. In th
Publikováno v:
Journal of the Japan Institute of Metals. 70:956-961
Titanium is used as an implant material for dentures. However, the corrosion caused by fluoride and the low wettability of titanium by saliva are still problems. In this study, the corrosion behavior of pure titanium and its alloy was investigated in
Publikováno v:
Journal of the Japan Institute of Metals. 70:929-935
Publikováno v:
Journal of the Japan Institute of Metals. 70:769-774
Recently, the use of soldering tips using Pb-free solder has caused problems because the Nickel- or Iron-plating layer on the soldering tip is easily eroded by the Pb-free solder. Therefore, solder tips with higher solder erosion resistance and wetta