Zobrazeno 1 - 10
of 117
pro vyhledávání: '"Faeghinia, A."'
Publikováno v:
In Results in Chemistry January 2024 7
Publikováno v:
Results in Chemistry, Vol 7, Iss , Pp 101347- (2024)
This paper analytically evaluates LiTiS2, NaTiS2, MgTiS2, AlTiS2, Al0.5TiS2, KTiS2, CaTiS2, and ZnTiS2 electrode materials, via DFT calculations, to use in Li-, Na-, Mg-, Al-, K-, Ca-, and Zn- ion intercalation batteries. The structural properties an
Externí odkaz:
https://doaj.org/article/7586ac7a1d2f450a898db2aaa656c5e4
Publikováno v:
In Optical Materials December 2023 146
Publikováno v:
In Journal of Energy Storage 1 December 2023 73 Part A
Autor:
Kouchaki Foroshani, A.H., Faeghinia, A., Afghahi, S. Seyed, Tayebifard, S.A., Sedaghat Ahangri Hossein Zadeh, A.
Publikováno v:
In Ceramics International 15 October 2022 48(20):29782-29789
Publikováno v:
Journal of Asian Ceramic Societies, Vol 9, Iss 1, Pp 30-39 (2021)
The corrosion resistance of the low-cement alumina base refractory against the slag of the electric arc furnace using zirconia was studied. Colloidal zirconia was replaced at the expense of the calcium aluminate cement by 1, 2, and 4 wt.% (C1, C2, an
Externí odkaz:
https://doaj.org/article/c43375077c0f4606925d9747ac821243
Publikováno v:
In Ceramics International 1 August 2020 46(11) Part B:19217-19227
Publikováno v:
In Journal of Luminescence May 2020 221
Autor:
Faeghinia A., Ebadzadeh T.
Publikováno v:
Science of Sintering, Vol 52, Iss 4, Pp 469-479 (2020)
In this work, Hydroxyapatite (HAp) was sintered by microwave and compared with the sintered samples by conventional method. The power levels of microwave were 450, 600, 900 W and the sintering temperatures were in the range from 750 to 1000 °C wi
Externí odkaz:
https://doaj.org/article/394d7215c025441eb98179b0cd54d900
Autor:
A. Faeghinia, H. Mardi
Publikováno v:
Journal of Advanced Materials in Engineering, Vol 38, Iss 4, Pp 51-64 (2020)
Amorphous steel slag was blended with different concentrations of waste glass (20, 40, 50, 60, 70 wt.%) and SiC to obtain a composite. According to Hot Stage Microscopy images, slag-glass composite contractions started at 1050 ºC. scanning electron
Externí odkaz:
https://doaj.org/article/b86f7b37a64f47e8a22d3bde4f63b884