The reliability of LEDs decreases in moist environments. One potential gateway of moisture ingress, reducing the product lifetime is the lens. In white LEDs, phosphor particles are embedded into the optical silicone of the lens to convert the blue li
Externí odkaz:
https://doaj.org/article/62aaf58c405b4738a7570b93f4e4cb25
Autor:
Johannes M. C. Mol, Annemarie Herrmann, W.D. van Driel, Balakrishnan Munirathinam, S.J.F. Erich, F. De Buyl, J.P.B. van Dam, Olaf C. G. Adan, L.G.J. van der Ven
Publikováno v:
Journal of Materials Science and Technology, 64, 203-213. Elsevier
Journal of Materials Science & Technology: an international journal in the field of materials science, 64
Journal of Materials Science & Technology: an international journal in the field of materials science, 64
In general, packaging materials which encapsulate light emitting diodes (LEDs) and microelectronic devices offer barrier protection against several environmental hazards such as water and ionic contaminants. However, these encapsulants may provide pa
Autor:
Johannes M. C. Mol, L.G.J. van der Ven, HP Henk Huinink, Ocg Olaf Adan, A. Herrmann, W.D. van Driel, M. van Soestbergen, S.J.F. Erich, F. De Buyl, A. Mavinkurve
Publikováno v:
Optical Materials: X, Vol 6, Iss, Pp-(2020)
Optical Materials: X, 6:100047. Elsevier
Optical Materials: X, 6
Optical Materials: X, 6:100047. Elsevier
Optical Materials: X, 6
The reliability of LEDs decreases in moist environments. One potential gateway of moisture ingress, reducing the product lifetime is the lens. In white LEDs, phosphor particles are embedded into the optical silicone of the lens to convert the blue li
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::639223197470c9b0a7d57a27dbd3ecfb
http://resolver.tudelft.nl/uuid:b79f7dae-89f0-4894-aed0-8b83db09ec92
http://resolver.tudelft.nl/uuid:b79f7dae-89f0-4894-aed0-8b83db09ec92
Autor:
Leendert G.J. van der Ven, A. Herrmann, W.D. van Driel, M. van Soestbergen, Olaf C. G. Adan, F. De Buyl, A. Mavinkurve, S.J.F. Erich
Publikováno v:
18th International Conference on Thermal, Mechanical and Multi-Physics Simulation and Experiments in Microelectronics and Microsystems, EuroSimE 2017. 3 April 2017 through 5 April 2017, 1-6
2017 18th International Conference on Thermal, Mechanical and Multi-Physics Simulation and Experiments in Microelectronics and Microsystems, EuroSimE 2017, 3-5 April 2017, Dresden, Germany
2017 18th International Conference on Thermal, Mechanical and Multi-Physics Simulation and Experiments in Microelectronics and Microsystems, EuroSimE 2017, 3-5 April 2017, Dresden, Germany
Tarnishing of the reflective silver layer in LED packages is an important failure mechanism, leading to both a decrease in luminous flux by up to 75% and a change in color spectrum.
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_dedup___::45ec0f6fefcba47073b416b74cbd6bb0
https://research.tue.nl/en/publications/0d06ff32-9be8-4bad-9317-7c964627b57f
https://research.tue.nl/en/publications/0d06ff32-9be8-4bad-9317-7c964627b57f
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Publikováno v:
International Journal of Adhesion and Adhesives. 22:331-336
PTFE tape can be placed in contact with silicone glazing sealants, before they cure by reaction with water vapour from the atmosphere. Upon removal of the tape after cure, a smooth and tack free silicone surface remains. This phenomenon has been inve
Publikováno v:
International Journal of Adhesion and Adhesives. 22:385-393
When an alkoxysilicone sealant is exposed to moist air, a surface skin is formed, which becomes thicker with time. It has been observed that, at constant temperature and humidity, the thickness (cure depth) is initially proportional to the square roo
Autor:
John Comyn, F. De Buyl
Publikováno v:
European Polymer Journal. 37:2385-2391
The water vapour permeability coefficient (P) of a silica reinforced siloxane network has been measured in the temperature range 5–45°C. P is independent of humidity and stretching of the material, but a plot of logP against reciprocal absolute te
Akademický článek
Tento výsledek nelze pro nepřihlášené uživatele zobrazit.
K zobrazení výsledku je třeba se přihlásit.
K zobrazení výsledku je třeba se přihlásit.
Publikováno v:
International Journal of Adhesion and Adhesives. 23:495-497
A method has been devised for measuring the diffusion coefficient D of additives that act as adhesion promoters and crosslinking agents in uncured silicone sealants. This has been used to measure D for tetra-t-butyltitanate (TBT) and isobutyltrimetho