Zobrazeno 1 - 10
of 19
pro vyhledávání: '"Fırat Karakaş"'
Publikováno v:
KONA Powder and Particle Journal, Vol 29, Iss 0, Pp 96-106 (2014)
Rheology plays a major role both in production and application stages of paints. Na-Bentonite, clay based thickening agent, is generally used to modify the viscosity of paints, since it is more economical and environmentally friendly compared to poly
Externí odkaz:
https://doaj.org/article/17893b82d13e4ecd8a58ac430875f2a9
Autor:
Fırat Karakaş, Mehmet S. Çelik
Publikováno v:
Progress in Organic Coatings. 123:292-298
Different types of minerals in varying amounts are used in paint formulations depending on the paint characteristic. While titanium dioxide (TiO 2 ) is used as a main pigment to improve the paint properties, some minerals such as calcite and calcined
Publikováno v:
International Journal of Coal Preparation and Utilization. 40:564-580
Fine and ultrafine coal (−200 µm) enrichment and its further dewatering processes are more difficult than that of coarser sizes. Utilization of this size fraction, however, is inevitable owing to e...
Publikováno v:
International Journal of Mineral Processing. 156:69-74
Morphological features of particles.upon size reduction affect flotation recoveries in terms of kinetics, bubble particle interactions and even suspension properties. The significance of surface roughness and shape factor of particles on flotation re
Autor:
Fırat Karakaş, Ahmad Hassanzadeh
Publikováno v:
Journal of Dispersion Science and Technology. 38:309-316
Obtaining high recovery in coarse particle size fractions has been always under investigation in recent years. In the present study, stage addition of chemical reagents is used to improve copper grade and recovery of coarse size fractions (i.e., >100
Autor:
Fırat Karakaş, Ahmad Hassanzadeh
Publikováno v:
Particulate Science and Technology. 35:455-461
In this study, a series of batch flotation experiments was conducted to evaluate both the role of particle size distribution and the presence of sodium metabisulfite Na2S2O5 (SMBS) in chalcopyrite and pyrite flotation. Kinetic flotation tests were al
Autor:
Fırat Karakaş, Behzad Vaziri Hassas, Onur Guven, Mustafa Cinar, Mehmet S. Çelik, Hidayet Caliskan
Publikováno v:
Colloids and Surfaces A: Physicochemical and Engineering Aspects. 492:88-99
The effect of surface roughness and shape factor on behavior of particles in flotation has been investigated. Surface roughness of various degrees was applied on spherical glass beads of −150 +106 μm by means of acid etching. The same procedure wa
Publikováno v:
Progress in Organic Coatings. 83:64-70
Titanium dioxide (TiO 2 ) due to its high refractive index, is widely used in paint industry as a white pigment. In order to reduce this high cost of TiO 2 , a part of TiO 2 is generally substituted by some other industrial mineral fillers such as ca
Publikováno v:
Minerals, Vol 7, Iss 11, p 223 (2017)
Minerals; Volume 7; Issue 11; Pages: 223
Minerals; Volume 7; Issue 11; Pages: 223
A theoretical analysis was conducted to study the role of collectors and depressants in flotation, based on the extended Derjaguin–Landau–Verwey–Overbeek (DLVO) theory, where the hydrophobic force is considered. The collector-coated hydrophilic
Publikováno v:
International Journal of Mineral Processing. 133:97-104
Dewatering process is one of the most costly steps in mineral processing and coal washing plants. This fact becomes an important industrial challenge in lignite cleaning. The presence of micropores and relatively low hydrophobic nature of lignitic co