Publikováno v:
Metal Science and Heat Treatment. 23:503-506
1. On the surface of titanium and its alloys nitrided at 900 and 1000° for 5–10 h a thin layer of titanium nitride is formed, a recrystallized layer of the solid solution of Tiα saturated with nitrogen, and TiN−Ti2N during the decomposistion of
Publikováno v:
Metal Science and Heat Treatment. 19:701-704
1. Annealing in air at 600 and 700° for as long as 100 h has little effect on the strength or ductility of alloy AT3 but lowers the ultimate strength and yield strength of alloy AT6 by 5–8 kgf/mm2. Annealing at 800° leads to a sharp reduction of
Publikováno v:
Metal Science and Heat Treatment. 21:394-396
1. The temperature and pH of the corrosive solution determine, while mineralization and the flow rate of the corrosive solution have no effect on, the gas-abrasive wear of alloys AT3 and AT6. 2. Wear is negligible in alkaline and neutral solutions at
Publikováno v:
Metal Science and Heat Treatment. 14:396-398
1. The scale resistance of Ti−Sn−O alloys at 700–1000o with up to 10%Sn and with 0.35% O indicates that the presence of oxygen in Ti−Sn alloys lowers the oxidation rate at all temperatures tested. However, the oxidation rate still tends to in
Publikováno v:
Metal Science and Heat Treatment. 12:243-245
1. In solid solutions of the Ti−Sn−O system the modulus of elasticity and characteristic temperature increases, while the rms deviation of atoms decreases, with increasing concentrations of oxygen. 2. There is a relationship between the strength