Publikováno v:
Metals, Vol 12, Iss 11, p 1877 (2022)
The fatigue behavior of the two austenitic stainless steels AISI 904L and AISI 347 with different surface morphologies, (i) conventionally turned and finally polished, (ii) cryogenic turned using CO2 snow, as well as (iii) cryogenic turned and finall
Externí odkaz:
https://doaj.org/article/a4367974d51644d3bdbae5fb68439ba6
Publikováno v:
Metals, Vol 12, Iss 7, p 1066 (2022)
For a reliable design of structural components, valid information about the fatigue strength of the material used is a prerequisite. As the determination of the fatigue properties, and especially the fatigue limit σw, requires a high experimental ef
Externí odkaz:
https://doaj.org/article/ae3f21c75eb4494295b6c307efa61f26
Publikováno v:
Mechanical Engineering Journal, Vol 3, Iss 6, Pp 16-00303-16-00303 (2016)
Alternatively to conventional stress-strain hysteresis measurements in this paper physically based materials data such as specimen temperature, electrical resistance, speed of sound or generator power are used to describe the cyclic deformation behav
Externí odkaz:
https://doaj.org/article/727ef5593e7a49b6bde14fd44d999af1
Autor:
Joachim E. Hoffmann, Vrushali Pawar, Dietmar Eifler, Tina Eyrisch, Torsten Hielscher, Monika Saumer, Patrick Klär, Martin-Tobias Schmitt, Peter Starke
Publikováno v:
Materials Testing. 64:903-931
Thin strips of electrochemically deposited nanocrystalline nickel-iron with thicknesses of 320 or 330 µm are modified by defined grinding. Small changes in the cutting depth and the variation of the grinding process, up cut or down cut, result in di
Autor:
Tina Eyrisch, Dietmar Eifler, Joachim E. Hoffmann, Monika Saumer, Tilmann Beck, Martin-T. Schmitt, Torsten Hielscher, Peter Starke, Patrick Klär
Publikováno v:
Materials Testing. 62:225-241
Nanocrystalline nickel-iron layers are produced electrochemically on copper discs by varying the current density and then annealed in a vacuum furnace at a temperature range between 200 and 800 °C. Grain size, iron content, texture and microstrain o
Publikováno v:
International Journal of Fatigue. 119:78-88
Short-time procedures for determining the fatigue properties of materials can provide significant improvements in cost efficiency and are therefore of great scientific and industrial interest (Jost et al., 2017). A promising short-time procedure is P
Publikováno v:
International Journal of Fatigue. 117:274-282
Components of internal combustion engines not only undergo mechanical high and low-cycle fatigue but also thermally induced loadings during start-stop and load changes. Accordingly, an efficient lifetime calculation method of the ductile cast iron EN
Autor:
Dietmar Eifler, Joachim E. Hoffmann, Patrick Klär, Monika Saumer, Tilmann Beck, Martin-T. Schmitt
Publikováno v:
Materials Testing. 60:1041-1049
Nanocrystalline nickel-iron microstructures, manufactured by means of an electrochemical deposition process via electrolyte solutions, were investigated to collect relevant information for the use of nickel-iron for micro-components. By varying the c
Autor:
Dietmar Eifler, Patrick Mayer, Christopher Müller, Marek Smaga, Ralf Müller, Hendrik Hotz, Tilmann Beck, Steven Becker, Robert Skorupski, Erik von Harbou, Benjamin Kirsch, Jan C. Aurich, Annika Boemke
Publikováno v:
CIRP Journal of Manufacturing Science and Technology. 23:6-19
In recent years, deformation induced surface hardening when turning was carried out to enhance the component performance of metastable austenitic steels. To induce such a phase transformation from austenite to martensite in the workpiece surface laye
Publikováno v:
Materials Testing. 60:669-677
Weight-optimized component design as well as a reliable estimation of the lifetime of metallic materials and components require a comprehensive understanding of fatigue processes and a systematic investigation of the underlying fatigue behavior. This