Zobrazeno 1 - 10
of 95
pro vyhledávání: '"Dayong Shan"'
Autor:
Dan Liu, Yuanjing Liu, Wei Yuan, Haitao Li, Xiong Huang, Zhiheng Zhang, Yinying Sheng, Zimin Li, Kaihui Dong, Wanqi Chen, Lan Cui, Dayong Shan
Publikováno v:
Nuclear Materials and Energy, Vol 39, Iss , Pp 101664- (2024)
Alternative to cyanide silver coatings with low infrared emissivity for tokamak components were prepared by cyanide-free silver plating on nuclear-grade 304L stainless steel. The surface morphology, coating adhesion and emissivity were characterized
Externí odkaz:
https://doaj.org/article/779d325c5647497c87b7e889822023be
Publikováno v:
Materials Research Express, Vol 11, Iss 5, p 056405 (2024)
Hydroxyethyl cellulose (HEC) has been commonly used in a variety of complex formulations for acid copper plating. However, the roles of HEC acting in acid copper plating still lacks of systematic investigation. To explore the efficacy of HEC in the d
Externí odkaz:
https://doaj.org/article/eaa672622ca7421d95357f18c0278c25
Publikováno v:
Journal of Magnesium and Alloys, Vol 9, Iss 4, Pp 1220-1232 (2021)
Coatings on the surface of Mg alloys are inevitably damaged during their practical applications, and corrosion can easily initiate from the damaged areas to accelerate the failure of Mg parts. A dual self-healing coating has already been developed to
Externí odkaz:
https://doaj.org/article/0523dd3cb82f4a409bc9a840122b8f5f
Publikováno v:
Journal of Magnesium and Alloys, Vol 5, Iss 1, Pp 26-34 (2017)
The influence of yttrium on the corrosion behavior of Mg–Y alloys has been investigated by electrochemical measurements, scanning electron microscope (SEM) observation, X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS) analysis in
Externí odkaz:
https://doaj.org/article/34fab6e7d8c04412afbd657049dee331
Publikováno v:
Acta Metallurgica Sinica (English Letters). 35:1559-1571
Publikováno v:
Electrochimica Acta. 454:142375
Publikováno v:
Journal of Magnesium and Alloys, Vol 9, Iss 4, Pp 1220-1232 (2021)
Coatings on the surface of Mg alloys are inevitably damaged during their practical applications, and corrosion can easily initiate from the damaged areas to accelerate the failure of Mg parts. A dual self-healing coating has already been developed to
Publikováno v:
Corrosion Communications. 2:24-32
Mg-3Zn alloy presents filiform corrosion in NaCl solution but pitting corrosion in Na2SO4 solution. The mechanisms for those different localized corrosion forms were investigated using SEM, XPS and electrochemical measurements. It is found that surfa
Publikováno v:
Journal of Magnesium and Alloys, Vol 2, Iss 3, Pp 208-213 (2014)
Hydrogen evolution reaction is inevitable during the corrosion of Mg alloys. The effect of hydrogen on the corrosion behavior of the Mg–2Zn and Mg–5Zn alloys is investigated by charging hydrogen treatment. The surface morphologies of the samples
Externí odkaz:
https://doaj.org/article/090ef1b3bc4c48ad954776cf9e3d2c7c
Publikováno v:
Journal of Materials Science. 56:3510-3524
The destruction of Ti passive film cannot occur if fluorine ions (F−) are below a critical concentration in an open electrolyte with oxygen acting as a passivating agent. However, in an occluded crevice, few F− combined with oxygen deficiency env