Zobrazeno 1 - 10
of 44
pro vyhledávání: '"D.S. Ramachandra Murthy"'
Autor:
P. Gandhi, D.S. Ramachandra Murthy, P.F. Anto, P.K. Pant, A.K. Samant, A. G. Madhava Rao, G. Raghava
Publikováno v:
Tubular Structures VI ISBN: 9780203735015
Fatigue cracks are found to appear in welded steel tubular joints of offshore structures during their service life necessitating costly repairs and maintenance. Two unstiffened and seven internally ring stiffened steel tubular joints were tested unde
Externí odkaz:
https://explore.openaire.eu/search/publication?articleId=doi_________::f1abad4cc5404ed7eab96298f70c5af2
https://doi.org/10.1201/9780203735015-94
https://doi.org/10.1201/9780203735015-94
Publikováno v:
Fatigue & Fracture of Engineering Materials and Structures. 30:1203-1213
Steam generators are important components of a nuclear reactor. They are subjected to system pressure and force controlled bending moments. Leak before break (LBB) criteria based on a fracture mechanics approach is used to ensure the reliability of t
Publikováno v:
Engineering Structures. 29:789-801
Ductile fracture assessments of circumferentially through-wall cracked piping components performed on the basis of the elastic–plastic J -integral concepts are discussed with particular interest in its ability and accuracy to predict actual experim
Publikováno v:
The Journal of Strain Analysis for Engineering Design. 41:525-537
Analysis and estimation of fracture parameters in flawed nuclear piping systems are of great importance in developing appropriate methodologies for ensuring structural integrity of these systems. The understanding of the response of surface-cracked p
Publikováno v:
The Journal of Strain Analysis for Engineering Design. 40:525-533
The study of crack growth is important to evaluate the structural integrity of nuclear power plant piping from the viewpoint of the leak-before-break concept. A thick-walled pipe with a semi-elliptical circumferential surface crack of different initi
Autor:
Suneel Gupta, D.S. Ramachandra Murthy, K.K. Vaze, H. S. Kushwaha, D. Venu Kumar, Vivek Bhasin, S. Seetharaman
Publikováno v:
Fatigue & Fracture of Engineering Materials & Structures. 27:1061-1072
Earthquake load, which is cyclic in nature and of short duration, is the main design basis accident load for designing the primary heat transport (PHT) piping components of Nuclear Power Plants. Adequate protection of piping components from the effec
Publikováno v:
Engineering Structures. 26:1165-1172
In order to evaluate the structural integrity of power plants, it is required to know the load carrying capacity of a piping system. J-integral based elastic-plastic fracture mechanics (EPFM) has become a useful analytical technique for dealing with
Publikováno v:
International Journal of Pressure Vessels and Piping. 80:629-640
Studies have been carried out on carbon steel pipes to demonstrate the leak before break design criterion and validate the analytical procedures. Fatigue crack initiation, fatigue crack growth rate and fracture resistance behaviour of the pipes have
Publikováno v:
Engineering Structures. 22:1390-1401
Welded steel tubular structures commonly used for offshore platforms are susceptible to fatigue failure due to stress concentration at welded joints and environmental loading which is cyclic in nature. Offshore structures contain flaws ranging from m
Publikováno v:
Journal of Structural Engineering. 126:809-815
The use of internal ring stiffeners in offshore steel jacket platforms is a subject of controversy because of their peculiar failure pattern, observed in several tests in the early 1980s. It is estimated that at least 2,000 internally ring-stiffened