The principal characteristics and parameters were determined for the production of ceramics from yttrium oxide by hot pressure-casting. The products sinter to a relative density of 97–99.5%. High-sintered yttrium oxide ceramic produced by hot press
Publikováno v:
Refractories. 15:233-238
The property indices of pure-mullite specimens are high and approach those of pure-oxide products, i.e., creep, volatility and the coefficient of thermal expansion are low, the high-temperature strength is good, spalling resistance is satisfactory, a
Publikováno v:
Glass and Ceramics. 34:240-244
Publikováno v:
Refractories. 20:438-442
The heat treatment at 2000°C of zirconia ceramic with a grainy structure causes the destabilization of the ZrO2-CaO solid solutions but this is not complete after a 200-h dwell; the electrosmelted ZrO2 ceramic stabilized with CaO is more stable unde
Autor:
D. N. Poluboyarinov, V. M. Tatarintsev, V. K. Garanin, I. A. Surkova, V. L. Balkevich, V. I. Aleksandrov, N. M. Nikitina, V. V. Osiko
Publikováno v:
Refractories. 18:230-235
The high-frequency smelting of a charge containing 69–75% Al2O3 and 31−25% SiO2 gives a product with a stable phase composition of mullite and glass. Corundum occurs only in the form of discrete crystals.
Publikováno v:
Refractories. 17:757-760
An investigation was carried out of the creep and long-term strength of Al2O3 ceramics with crystal sizes of 15–20 and 30–35μ at 1400–1550°C and stresses of 100–500 kgf/cm2. The test conditions remaining the same, the ceramic with the small
Publikováno v:
Refractories. 15:301-304
Scandium oxide consists of aggregations of crystals of various sizes. Protracted wet grinding in a ball mill breaks up the aggregations to give a finely dispersed powder. The density of the moldings depends essentially on the molding pressure and var
Autor:
D. N. Poluboyarinov, I. G. Kuznetsova
Publikováno v:
Refractories. 8:190-195
During hot pressing only powders of BN synthesized at low temperatures are sintered. The high dispersion of the powder, and the imperfect structure of the crystals lead to its recrystallization and sintering at high temperatures.