Zobrazeno 1 - 10
of 13
pro vyhledávání: '"D. M. Petergerya"'
Publikováno v:
Soviet Materials Science. 4:374-377
Vacuum diffusion chromizing was studied as a method of increasing fatigue strength and the corrosion and erosion resistance of steel. It was shown that carbon steels chromized by this method can be used in place of stainless chromium-nickel steels.
Publikováno v:
Soviet Materials Science. 8:654-657
Autor:
A. A. Domio, V. G. Kas'yanenko, P. A. Mikhailov, V. F. Rybkin, V. P. Khokhlov, D. M. Petergerya, E. P. Ponomarenko
Publikováno v:
Soviet Materials Science. 4:94-97
The fatigue strength and wear resistance of steels St. 3, P-1, EI-802, and EI-612 after vacuum-diffusion chromizing, siliciding and boriding was studied. It was shown that the wear resistance of carbon steels is increased more than 20-fold by boridin
Autor:
D. M. Petergerya, I. G. Fridlender
Publikováno v:
Metal Science and Heat Treatment. 6:11-15
1. Discs made of the KhN77TYuR alloy should be annealed for 8h at 750°C. Argon is the best annealing medium; it ensures the required mechanical properties. In the case of blades, annealing in argon or nitrogen increases the fatigue limit, the impact
Publikováno v:
Strength of Materials. 7:16-18
Autor:
D. M. Petergerya
Publikováno v:
Metal Science and Heat Treatment. 8:38-40
Autor:
L. E. Zakharenko, S. Ya. Panfilova, D. M. Petergerya, Yu. K. Belov, M. P. Borisenko, E. P. Ponomarenko
Publikováno v:
Soviet Materials Science. 7:594-596
Autor:
G. P. Khoroshailo, E. P. Ponomarenko, P. A. Mikhailov, V. F. Rybkin, L. I. Filina, V. P. Khokhlov, D. M. Petergerya
Publikováno v:
Soviet Materials Science. 4:98-100
It was established that vacuum-diffusion contactless manganizing and chromizing produces a 2.5 to 3-fold increase in the wear resistance of a titanium alloy VT-8, whose fatigue strength is reduced by 50% after these treatments due to a columnar grain
Autor:
D. M. Petergerya, V. K. Yatsenko
Publikováno v:
Soviet Materials Science. 13:551-552
Specimens 7.5 mm in diameter , which were prepared f rom a hot-rolled rod 20 mm in diameter , p o s sessed a hardness ranging f rom BHN = 290-320 af ter heat t reatment . The preground specimens were bur nishedwith adtamondhavtng: a spher ical radius
Publikováno v:
Soviet Materials Science. 9:477-478